Use of carbonated calcium rich waste material in composite binders as component of building materials hardened by carbonation to make a building structure wherein the composite binder is made by mixing from 5 to 75 wt.-% carbonated calcium rich waste material and from 20 to 95 wt.-% of at least one calcium silicate with the sum of their amounts ranging from 50 to 100 wt.-% of the composite binder and the carbonated calcium rich waste material contains at least 10 wt.-% calcium calculated as CaO determined by X-ray fluorescence, the building material is made by mixing the composite binder with water or an aqueous liquid, and the building material is hardened by carbonation at a CO2 concentration from 1 to 99 Vol.-% to provide the building structure, as well as method for building a building structure comprising manufacturing building materials adapted to harden by carbonation by mixing carbonated calcium rich waste material with at least one calcium silicate to provide a composite binder hardened by carbonation.
L'invention concerne l'utilisation de déchets riches en calcium carbonaté dans des liants composites en tant que constituant de matériaux de construction durcis par carbonatation pour fabriquer une structure de construction, le liant composite étant préparé par mélange de 5 à 75 % en poids de déchets riches en calcium carbonaté et de 20 à 95 % en poids d'au moins un silicate de calcium, la somme de leurs quantités allant de 50 à 100 % en poids du liant composite, et les déchets riches en calcium carbonaté contenant au moins 10 % en poids de calcium, calculés sous forme de CaO, déterminés par fluorescence de rayons X, le matériau de construction étant préparé par mélange du liant composite avec de l'eau ou un liquide aqueux et le matériau de construction étant durci par carbonatation à une concentration en CO2 de 1 à 99 % en volume pour obtenir la structure de construction. L'invention concerne également un procédé de construction d'une structure de construction comprenant la fabrication de matériaux de construction conçus pour durcir par carbonatation par mélange des déchets riches en calcium carbonaté avec au moins un silicate de calcium pour obtenir un liant composite durci par carbonatation.
Use of carbonated calcium rich waste material in composite binders as component of building materials hardened by carbonation to make a building structure wherein the composite binder is made by mixing from 5 to 75 wt.-% carbonated calcium rich waste material and from 20 to 95 wt.-% of at least one calcium silicate with the sum of their amounts ranging from 50 to 100 wt.-% of the composite binder and the carbonated calcium rich waste material contains at least 10 wt.-% calcium calculated as CaO determined by X-ray fluorescence, the building material is made by mixing the composite binder with water or an aqueous liquid, and the building material is hardened by carbonation at a CO2 concentration from 1 to 99 Vol.-% to provide the building structure, as well as method for building a building structure comprising manufacturing building materials adapted to harden by carbonation by mixing carbonated calcium rich waste material with at least one calcium silicate to provide a composite binder hardened by carbonation.
L'invention concerne l'utilisation de déchets riches en calcium carbonaté dans des liants composites en tant que constituant de matériaux de construction durcis par carbonatation pour fabriquer une structure de construction, le liant composite étant préparé par mélange de 5 à 75 % en poids de déchets riches en calcium carbonaté et de 20 à 95 % en poids d'au moins un silicate de calcium, la somme de leurs quantités allant de 50 à 100 % en poids du liant composite, et les déchets riches en calcium carbonaté contenant au moins 10 % en poids de calcium, calculés sous forme de CaO, déterminés par fluorescence de rayons X, le matériau de construction étant préparé par mélange du liant composite avec de l'eau ou un liquide aqueux et le matériau de construction étant durci par carbonatation à une concentration en CO2 de 1 à 99 % en volume pour obtenir la structure de construction. L'invention concerne également un procédé de construction d'une structure de construction comprenant la fabrication de matériaux de construction conçus pour durcir par carbonatation par mélange des déchets riches en calcium carbonaté avec au moins un silicate de calcium pour obtenir un liant composite durci par carbonatation.
COMPOSITE BINDER HARDENING BY CARBONATION
DURCISSEMENT DE LIANT COMPOSITE PAR CARBONATATION
ZAJAC MACIEJ (author)
2024-06-06
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
The hardening behavior of γ-C2S binder using accelerated carbonation
British Library Online Contents | 2016
|The hardening behavior of γ-C2S binder using accelerated carbonation
Online Contents | 2016
|The hardening behavior of γ-C2S binder using accelerated carbonation
British Library Online Contents | 2016
|The hardening behavior of [gamma]-[C.sub.2]S binder using accelerated carbonation
Online Contents | 2016
|