METHOD FOR PRODUCING RECYCLED ZIRCONIA
The present invention provides at least one of: a method for producing, from a zirconia sintered body, recycled zirconia that can be easily pulverized; and a zirconia sintered body recycling method capable of recycling a zirconia sintered body. This method for producing recycled zirconia comprises an ammonia treatment step for heat-treating a zirconia sintered body at a temperature of 800-1200°C in an oxygen-containing ammonia atmosphere. The ammonia treatment step satisfies either one of condition (a) or condition (b). (a) The concentration of oxygen in the oxygen-containing ammonia atmosphere is at least 0.3 vol%. (b) The concentration of oxygen in the oxygen-containing ammonia atmosphere is at least 0.2 vol%, and the cubic crystal ratio of the zirconia sintered body is at least 3.5%.
La présente invention concerne au moins l'un parmi : un procédé de production, à partir d'un corps fritté de zircone, de zircone recyclée qui peut être facilement pulvérisée ; et un procédé de recyclage de corps fritté de zircone capable de recycler un corps fritté de zircone. Ce procédé de production de zircone recyclée comprend une étape de traitement à l'ammoniac permettant le traitement thermique d'un corps fritté de zircone à une température de 800 à 1200°C dans une atmosphère d'ammoniac contenant de l'oxygène. L'étape de traitement à l'ammoniac satisfait l'un ou l'autre de la condition (a) ou de la condition (b) : (a) la concentration d'oxygène dans l'atmosphère d'ammoniac contenant de l'oxygène est d'au moins 0,3% en volume ; et (b) la concentration d'oxygène dans l'atmosphère d'ammoniac contenant de l'oxygène est d'au moins 0,2 % en volume, et le rapport de cristaux cubiques du corps fritté de zircone est d'au moins 3,5 %.
ジルコニア焼結体から粉砕しやすいリサイクルジルコニアを製造する方法、及び、ジルコニア焼結体をリサイクルできるジルコニア焼結体のリサイクル方法の少なくともいずれかを提供する。 酸素含有アンモニア雰囲気において、800℃以上1200℃以下の温度で、ジルコニア焼結体を熱処理するアンモニア処理工程を有し、前記アンモニア処理工程が、下記条件(a)と下記条件(b)のいずれか一方を満たす、リサイクルジルコニアの製造方法。 (a)前記酸素含有アンモニア雰囲気の酸素濃度が0.3体積%以上である。 (b)前記酸素含有アンモニア雰囲気の酸素濃度が0.2体積%以上であり、且つ、前記ジルコニア焼結体の立方晶率が3.5%以上である。
METHOD FOR PRODUCING RECYCLED ZIRCONIA
The present invention provides at least one of: a method for producing, from a zirconia sintered body, recycled zirconia that can be easily pulverized; and a zirconia sintered body recycling method capable of recycling a zirconia sintered body. This method for producing recycled zirconia comprises an ammonia treatment step for heat-treating a zirconia sintered body at a temperature of 800-1200°C in an oxygen-containing ammonia atmosphere. The ammonia treatment step satisfies either one of condition (a) or condition (b). (a) The concentration of oxygen in the oxygen-containing ammonia atmosphere is at least 0.3 vol%. (b) The concentration of oxygen in the oxygen-containing ammonia atmosphere is at least 0.2 vol%, and the cubic crystal ratio of the zirconia sintered body is at least 3.5%.
La présente invention concerne au moins l'un parmi : un procédé de production, à partir d'un corps fritté de zircone, de zircone recyclée qui peut être facilement pulvérisée ; et un procédé de recyclage de corps fritté de zircone capable de recycler un corps fritté de zircone. Ce procédé de production de zircone recyclée comprend une étape de traitement à l'ammoniac permettant le traitement thermique d'un corps fritté de zircone à une température de 800 à 1200°C dans une atmosphère d'ammoniac contenant de l'oxygène. L'étape de traitement à l'ammoniac satisfait l'un ou l'autre de la condition (a) ou de la condition (b) : (a) la concentration d'oxygène dans l'atmosphère d'ammoniac contenant de l'oxygène est d'au moins 0,3% en volume ; et (b) la concentration d'oxygène dans l'atmosphère d'ammoniac contenant de l'oxygène est d'au moins 0,2 % en volume, et le rapport de cristaux cubiques du corps fritté de zircone est d'au moins 3,5 %.
ジルコニア焼結体から粉砕しやすいリサイクルジルコニアを製造する方法、及び、ジルコニア焼結体をリサイクルできるジルコニア焼結体のリサイクル方法の少なくともいずれかを提供する。 酸素含有アンモニア雰囲気において、800℃以上1200℃以下の温度で、ジルコニア焼結体を熱処理するアンモニア処理工程を有し、前記アンモニア処理工程が、下記条件(a)と下記条件(b)のいずれか一方を満たす、リサイクルジルコニアの製造方法。 (a)前記酸素含有アンモニア雰囲気の酸素濃度が0.3体積%以上である。 (b)前記酸素含有アンモニア雰囲気の酸素濃度が0.2体積%以上であり、且つ、前記ジルコニア焼結体の立方晶率が3.5%以上である。
METHOD FOR PRODUCING RECYCLED ZIRCONIA
PROCÉDÉ DE PRODUCTION DE ZIRCONE RECYCLÉE
リサイクルジルコニアの製造方法
OHASHI NAOKI (author) / SEGAWA HIROYO (author) / KUBOTA AYUMU (author) / TSUCHIYA SATOSHI (author) / KOBAYASHI WATARU (author)
2024-10-03
Patent
Electronic Resource
Japanese
European Patent Office | 2021
|European Patent Office | 2022
|European Patent Office | 2020
|European Patent Office | 2022
|European Patent Office | 2024
|