During the fall of 1969 transverse cracks were sealed in a 13-mile section of bituminous pavement. Five hot-poured rubber asphalt sealers, three tack coat materials for priming the crack sidewall, a bond breaker and 40 different application procedures were used. Test sections were established to evaluate the materials and procedures. Field surveys were conducted to determine the amount of footage failed. Reference pins were also installed to measure crack movement. The field results were used to evaluate the materials and procedures incorporated in the study program.
During the fall of 1969 transverse cracks were sealed in a 13-mile section of bituminous pavement. Five hot-poured rubber asphalt sealers, three tack coat materials for priming the crack sidewall, a bond breaker and 40 different application procedures were used. Test sections were established to evaluate the materials and procedures. Field surveys were conducted to determine the amount of footage failed. Reference pins were also installed to measure crack movement. The field results were used to evaluate the materials and procedures incorporated in the study program.
Sealing Cracks in Bituminous Pavement
R. O. Wolters (author)
1973
41 pages
Report
No indication
English
Sealing Cracks in Bituminous Overlays of Rigid Bases
NTIS | 1984
|European Patent Office | 2021
|Bituminous Pavement Rejuvenator
NTIS | 1986
|Bituminous penetration pavement
Engineering Index Backfile | 1928
|Bituminous penetration pavement
Engineering Index Backfile | 1927
|