Abstract Laboratory tests were conducted on a reddish-brown lateritic soil treated with up to 12 % bagasse ash to assess its suitability in waste containment barriers applications. Soil samples were prepared using four compaction energies (i.e. reduced Proctor, standard Proctor, West African Standard or ‘intermediate’ and modified Proctor) at −2, 0, 2 and 4 % moulding water content of the optimum moisture content (OMC). Index properties, hydraulic conductivity (k), volumetric shrinkage and unconfined compressive strength (UCS) tests were performed. Overall acceptable zones under which the material is suitable as a barrier material were obtained. Results recorded showed improved index properties; hydraulic conductivity and UCS with bagasse ash treatment up to 8 % at the OMC. Volumetric shrinkage strain increased with higher bagasse ash treatment. Based on the overall acceptable zone obtained, an 8 % optimal bagasse ash treatment of the natural lateritic soil makes it suitable for use in waste containment barrier application.
Evaluation of bagasse ash treated lateritic soil as a potential barrier material in waste containment application
Abstract Laboratory tests were conducted on a reddish-brown lateritic soil treated with up to 12 % bagasse ash to assess its suitability in waste containment barriers applications. Soil samples were prepared using four compaction energies (i.e. reduced Proctor, standard Proctor, West African Standard or ‘intermediate’ and modified Proctor) at −2, 0, 2 and 4 % moulding water content of the optimum moisture content (OMC). Index properties, hydraulic conductivity (k), volumetric shrinkage and unconfined compressive strength (UCS) tests were performed. Overall acceptable zones under which the material is suitable as a barrier material were obtained. Results recorded showed improved index properties; hydraulic conductivity and UCS with bagasse ash treatment up to 8 % at the OMC. Volumetric shrinkage strain increased with higher bagasse ash treatment. Based on the overall acceptable zone obtained, an 8 % optimal bagasse ash treatment of the natural lateritic soil makes it suitable for use in waste containment barrier application.
Evaluation of bagasse ash treated lateritic soil as a potential barrier material in waste containment application
Eberemu, Adrian O. (author)
Acta Geotechnica ; 8 ; 407-421
2013-02-05
15 pages
Article (Journal)
Electronic Resource
English
Bagasse ash , Compaction , Hydraulic conductivity , Lateritic soil , Liner , Unconfined compressive strength , Volumetric shrinkage Engineering , Geoengineering, Foundations, Hydraulics , Continuum Mechanics and Mechanics of Materials , Geotechnical Engineering & Applied Earth Sciences , Soil Science & Conservation , Soft and Granular Matter, Complex Fluids and Microfluidics , Structural Mechanics
British Library Online Contents | 2013
|British Library Conference Proceedings | 2014
|Unsaturated Hydraulic Conductivity of Compacted Lateritic Soil Treated with Bagasse Ash
British Library Conference Proceedings | 2010
|