Influence of Rubber Powder Content on High-Temperature Performance of TOR Rubber Asphalt
Six kinds of TOR rubber asphalts with 5%-30% rubber powder contents of were selected to carry out conventional high-temperature tests and dynamic shear rheological tests to obtain some parameters reflecting the high-temperature performance of asphalt binders, such as softening point, dynamic viscosity at 60°C, rutting factor (G*/sinδ) at 60°C and critical temperature of rutting factor (TG*/sinδ). The results show that the changing tendency of two rheological parameters of TOR rubber asphalts, G*/sinδ at 60°C and TG*/sinδ, is ascend in first and descend at last with the increase of rubber powder content proportion. The high-temperature performance of TOR rubber asphalt with the rubber powder content about 20% is the best. Softening point and dynamic viscosity at 60°C, as two conventional high-temperature parameters of asphalt binders, can describe the high-temperature performance of TOR rubber asphalt with the rubber powder content below 20%, but cannot evaluate accurately the high-temperature performance of TOR rubber asphalt with the rubber powder content above 20%, because TOR rubber asphalt has formed a network structure at this moment.
Influence of Rubber Powder Content on High-Temperature Performance of TOR Rubber Asphalt
Six kinds of TOR rubber asphalts with 5%-30% rubber powder contents of were selected to carry out conventional high-temperature tests and dynamic shear rheological tests to obtain some parameters reflecting the high-temperature performance of asphalt binders, such as softening point, dynamic viscosity at 60°C, rutting factor (G*/sinδ) at 60°C and critical temperature of rutting factor (TG*/sinδ). The results show that the changing tendency of two rheological parameters of TOR rubber asphalts, G*/sinδ at 60°C and TG*/sinδ, is ascend in first and descend at last with the increase of rubber powder content proportion. The high-temperature performance of TOR rubber asphalt with the rubber powder content about 20% is the best. Softening point and dynamic viscosity at 60°C, as two conventional high-temperature parameters of asphalt binders, can describe the high-temperature performance of TOR rubber asphalt with the rubber powder content below 20%, but cannot evaluate accurately the high-temperature performance of TOR rubber asphalt with the rubber powder content above 20%, because TOR rubber asphalt has formed a network structure at this moment.
Influence of Rubber Powder Content on High-Temperature Performance of TOR Rubber Asphalt
Applied Mechanics and Materials ; 405-408 ; 1753-1756
2013-09-03
4 pages
Article (Journal)
Electronic Resource
English
Influence of Rubber Powder Content on High-Temperature Performance of TOR Rubber Asphalt
Tema Archive | 2013
|Influence of Rubber Powder Content on High-Temperature Performance of TOR Rubber Asphalt
British Library Conference Proceedings | 2013
|Performance Evaluation of Rubber Asphalt and Desulfurized Rubber Asphalt
Springer Verlag | 2025
|European Patent Office | 2023
|