Hydrogen Evolution and Early Blistering from Magnesium-Rich Primers on AA2024-T3
Hydrogen Evolution and Early Blistering from Magnesium-Rich Primers on AA2024-T3
Hydrogen Evolution and Early Blistering from Magnesium-Rich Primers on AA2024-T3
Lin, Junren (Autor:in) / Upadhyay, Vinod (Autor:in) / Qi, Xiaoning (Autor:in) / Battocchi, Dante (Autor:in) / Bierwagen, Gordon P. (Autor:in)
Corrosion ; 72 ; 377-383
01.01.2016
7 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11223
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Behavior of Magnesium-Rich Primers on AA2024-T3
British Library Online Contents | 2011
|British Library Online Contents | 2018
|Use of Magnesium Alloys as Pigments in Magnesium-Rich Primers for Protecting Aluminum Alloys
British Library Online Contents | 2009
|Hydrogen-induced cracking and blistering in -brass
British Library Online Contents | 1998
|Investigation of hydrogen implantation-induced blistering in SiGe
British Library Online Contents | 2005
|