Prochnost aglomerata iz rud KMA
Strength of sinter from KMA ores; greatest strength is possessed by sinter with uniformly-distributed pores not exceeding 5 mm in size; strength of sinter with basicity of 0.7 to 1.5 decreases because of multiple-phase microstructure; strong ferruginous fluxes with basicity of 5.0 can be obtained from KMA concentrates and Lebedinsk ore. (See also Stal n 5 May 1965 p 385-92)
Prochnost aglomerata iz rud KMA
Strength of sinter from KMA ores; greatest strength is possessed by sinter with uniformly-distributed pores not exceeding 5 mm in size; strength of sinter with basicity of 0.7 to 1.5 decreases because of multiple-phase microstructure; strong ferruginous fluxes with basicity of 5.0 can be obtained from KMA concentrates and Lebedinsk ore. (See also Stal n 5 May 1965 p 385-92)
Prochnost aglomerata iz rud KMA
Prochnost aglomerata iz rud KMA
Bazilevich, S.V. (Autor:in) / Kutsenko, V.F. (Autor:in) / Bazilevich, T.N. (Autor:in)
1965
6 pages
Aufsatz (Zeitschrift)
Englisch
© Metadata Copyright Elsevier B. V. All rights reserved.
Prochnost fibrobetona, armirovannogo razlichnymi voloknami
Tema Archiv | 1989
|Prochnost izgibaemykh zhelezobetonnykh elementove, etc
Engineering Index Backfile | 1965
|Prochnost vyderzhivaemogo pri razlichnykh temperatyrakh betona
Tema Archiv | 1986
|Prochnost stykovykh soedinenii seismostoikikh krupnopanel'nykh zdanii pri sdvige
Engineering Index Backfile | 1968
|