Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
The invention discloses high-performance light castable. The high-performance light castable comprises, according to the proportion, 35-45 parts of alumina clinker, 15-25 parts of alumina micro powder, 15-35 parts of mullite, 15-25 parts of monox powder, 2-5 parts of liquid water glass, 15-25 parts of sodium silicate-bonded sand, 3-7 parts of silicon iron powder, 4-10 parts of composite cement, 6-17 parts of shale ceramisite, 25-55 parts of high-poly aluminum chloride light balls, 5-8 parts of polystyrene small balls, 1-5 parts of carbon black, 10-25 parts of expanded perlite and 3-7 parts of floating beads. The high-performance light castable has the advantages of being light in weight, high in pressure resistance, insulated, resistant to acid, resistant to acid gas corrosion and the like.
The invention discloses high-performance light castable. The high-performance light castable comprises, according to the proportion, 35-45 parts of alumina clinker, 15-25 parts of alumina micro powder, 15-35 parts of mullite, 15-25 parts of monox powder, 2-5 parts of liquid water glass, 15-25 parts of sodium silicate-bonded sand, 3-7 parts of silicon iron powder, 4-10 parts of composite cement, 6-17 parts of shale ceramisite, 25-55 parts of high-poly aluminum chloride light balls, 5-8 parts of polystyrene small balls, 1-5 parts of carbon black, 10-25 parts of expanded perlite and 3-7 parts of floating beads. The high-performance light castable has the advantages of being light in weight, high in pressure resistance, insulated, resistant to acid, resistant to acid gas corrosion and the like.
High-performance light castable
CHEN WEIYU (Autor:in)
30.09.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME