Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
The invention relates to a method for preparing non-sintered ceramsite by adding dredged sludge. The method comprises the following steps: (1) pre-treatment of the dredged sludge; (2) material preparation: mixing and stirring smashed dredged sludge, cement, quick lime, gypsum and coal ash to prepare a dry mixture; the mass portions of the smashed dredged sludge, cement, quick lime, gypsum and coal ash are as follows: 60 to 80 parts of the dredged sludge, 1 to 6 parts of the cement, 1 to 6 parts of the quick lime, 1 to 6 parts of the gypsum and 3 to 15 parts of the coal ash; then uniformly mixing water glass with water to obtain a mixed solution of the water glass and the water, wherein the mass ratio of the adding amount of the water glass to the dredged sludge is 3 to 15: 60 to 80, and the adding amount of the water accounts for 40 to 60 percent of the total mass of the dry mixture and the water glass; (3) disc granulation; (4) primary curing of a product; (5) waterproofing work; (6) ultimate curing of the product, namely obtaining a finish product of the non-sintered ceramsite. According to the method provided by the invention, a large amount of dredged sludge can be added, the purpose of utilizing waste materials is realized, the requirements of a dredging Industry are met, the production energy consumption is low, and the produced non-sintered ceramsite can meet the demands of construction market.
The invention relates to a method for preparing non-sintered ceramsite by adding dredged sludge. The method comprises the following steps: (1) pre-treatment of the dredged sludge; (2) material preparation: mixing and stirring smashed dredged sludge, cement, quick lime, gypsum and coal ash to prepare a dry mixture; the mass portions of the smashed dredged sludge, cement, quick lime, gypsum and coal ash are as follows: 60 to 80 parts of the dredged sludge, 1 to 6 parts of the cement, 1 to 6 parts of the quick lime, 1 to 6 parts of the gypsum and 3 to 15 parts of the coal ash; then uniformly mixing water glass with water to obtain a mixed solution of the water glass and the water, wherein the mass ratio of the adding amount of the water glass to the dredged sludge is 3 to 15: 60 to 80, and the adding amount of the water accounts for 40 to 60 percent of the total mass of the dry mixture and the water glass; (3) disc granulation; (4) primary curing of a product; (5) waterproofing work; (6) ultimate curing of the product, namely obtaining a finish product of the non-sintered ceramsite. According to the method provided by the invention, a large amount of dredged sludge can be added, the purpose of utilizing waste materials is realized, the requirements of a dredging Industry are met, the production energy consumption is low, and the produced non-sintered ceramsite can meet the demands of construction market.
Method for preparing non-sintered ceramsite by adding dredged sludge
11.11.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
Dredged sludge non-sintered ceramsite and preparation method thereof
Europäisches Patentamt | 2021
|Method for preparing sludge ceramsite from domestic sludge
Europäisches Patentamt | 2022
|Method for preparing porous ceramsite from sludge and obtained porous ceramsite
Europäisches Patentamt | 2022
|Industrial sludge sintered ceramsite and preparation method thereof
Europäisches Patentamt | 2020
|