Method for comprehensively utilizing waste concrete and sludge to produce ecologic clinker
A method for comprehensively utilizing waste concrete and sludge to produce ecologic clinker is characterized in that the ecologic silicate clinker is prepared from waste concrete, sludge, a correction material and an alteration agent through a dry rotary kiln production line technology. The method concretely comprises the following steps: 1, preparing materials; 2, proportioning: carrying out microcomputer proportioning according to the following proportions: waste concrete 70-82%, sludge 10-20%, correction material 0-15% and alteration agent 0.5-3.0%, wherein the sum of the proportions of the materials is 100%; 3, pulverizing: grinding the above obtained mixed material by a vertical raw material milling system to obtain a powdery waste raw material with the 80[mu]m screen residue rate being not greater than 18%; and 4, calcining: sending the powdery waste raw material into a dry rotary kiln system, and calcining at 1350-1450DEG C for 20-45min. The method fully utilizes the most widespread and maximum limestone coarse aggregate waste concrete, sludge and other wastes, and benefits transition of a cement enterprise to green and environmentally-friendly industry.
Method for comprehensively utilizing waste concrete and sludge to produce ecologic clinker
A method for comprehensively utilizing waste concrete and sludge to produce ecologic clinker is characterized in that the ecologic silicate clinker is prepared from waste concrete, sludge, a correction material and an alteration agent through a dry rotary kiln production line technology. The method concretely comprises the following steps: 1, preparing materials; 2, proportioning: carrying out microcomputer proportioning according to the following proportions: waste concrete 70-82%, sludge 10-20%, correction material 0-15% and alteration agent 0.5-3.0%, wherein the sum of the proportions of the materials is 100%; 3, pulverizing: grinding the above obtained mixed material by a vertical raw material milling system to obtain a powdery waste raw material with the 80[mu]m screen residue rate being not greater than 18%; and 4, calcining: sending the powdery waste raw material into a dry rotary kiln system, and calcining at 1350-1450DEG C for 20-45min. The method fully utilizes the most widespread and maximum limestone coarse aggregate waste concrete, sludge and other wastes, and benefits transition of a cement enterprise to green and environmentally-friendly industry.
Method for comprehensively utilizing waste concrete and sludge to produce ecologic clinker
YIN WUJI (Autor:in) / YIN XIAOLIN (Autor:in)
09.12.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2021
|Method for producing ecologic cement and active sand by using waste concrete and sludge
Europäisches Patentamt | 2015
|Method for preparing artificial stone by comprehensively utilizing granite waste
Europäisches Patentamt | 2024
|Method for preparing foamed ceramic by comprehensively utilizing solid waste
Europäisches Patentamt | 2023
|