Light insulating brick
The present invention discloses a light insulating brick. The light insulating brick is prepared from the following main raw materials: 50% to 76% of industrial cinder, 6% to 20% of mud, 4% to 20% of potassium feldspar, 4% to 20% of albite, 4% to 20% of quartz and 0 to 15% of polished residues. According to the light insulating brick, the industrial cinder is taken as a main formula body, and the addition is more than 50%; and moreover, the whole sintering time of the light insulating brick is controlled within 4-7 hours. The prepared light insulating brick is rigid in texture, low in specific gravity and high in porosity, and the refractory temperature is over 1000 DEG C, so that conventional fire can be resisted easily; and the light insulating brick is low in heat conductivity and high in compressive strength, and is very suitable for heat insulation of outer walls and indoor heat insulation and sound insulation.
Light insulating brick
The present invention discloses a light insulating brick. The light insulating brick is prepared from the following main raw materials: 50% to 76% of industrial cinder, 6% to 20% of mud, 4% to 20% of potassium feldspar, 4% to 20% of albite, 4% to 20% of quartz and 0 to 15% of polished residues. According to the light insulating brick, the industrial cinder is taken as a main formula body, and the addition is more than 50%; and moreover, the whole sintering time of the light insulating brick is controlled within 4-7 hours. The prepared light insulating brick is rigid in texture, low in specific gravity and high in porosity, and the refractory temperature is over 1000 DEG C, so that conventional fire can be resisted easily; and the light insulating brick is low in heat conductivity and high in compressive strength, and is very suitable for heat insulation of outer walls and indoor heat insulation and sound insulation.
Light insulating brick
LIN ZHI (Autor:in) / WU ZHEN (Autor:in) / SHAO JUNJIE (Autor:in) / GUO FENG (Autor:in) / CHEN QUANDI (Autor:in)
23.12.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME