Firebrick dust-containing aerated building block and making method thereof
The invention discloses a firebrick dust-containing aerated building block and a making method thereof. The aerated building block is made from, by weight, 12-23 parts of silicon-calcium slag, 24-37 parts of firebrick dusts, 26-39 parts of Portland cement, 19-35 parts of gangue, 14-26 parts of anorthite, 18-32 parts of porous ceramsite, 28-42 parts of flue dust, 6-12 parts of locust bean gum, 10-15 parts of boron slag, 16-28 parts of blast furnace water quenching slag, 4-8 parts of sodium tripolyphosphate, 3-4 parts of silicon-aluminum alloy powder, 1-2 parts of sodium peroxide and a proper amount of water. The firebrick dusts added in the invention cooperate with gangue, anorthite and silicon-calcium slag to improve the mechanical performances, the acid and alkali corrosion resistance and the weatherability of the aerated building block, and cooperate with the porous ceramsite, the boron slag and the blast furnace water quenching slag to improve the fire resistance and the heat insulation property of the aerated building block. The aerated building block made in the invention has the advantages of excellent comprehensive performances, excellent mechanical performances, excellent weatherability, excellent acid and alkali corrosion resistance, excellent ageing crack resistance, excellent heat insulation property and excellent fire resistance.
Firebrick dust-containing aerated building block and making method thereof
The invention discloses a firebrick dust-containing aerated building block and a making method thereof. The aerated building block is made from, by weight, 12-23 parts of silicon-calcium slag, 24-37 parts of firebrick dusts, 26-39 parts of Portland cement, 19-35 parts of gangue, 14-26 parts of anorthite, 18-32 parts of porous ceramsite, 28-42 parts of flue dust, 6-12 parts of locust bean gum, 10-15 parts of boron slag, 16-28 parts of blast furnace water quenching slag, 4-8 parts of sodium tripolyphosphate, 3-4 parts of silicon-aluminum alloy powder, 1-2 parts of sodium peroxide and a proper amount of water. The firebrick dusts added in the invention cooperate with gangue, anorthite and silicon-calcium slag to improve the mechanical performances, the acid and alkali corrosion resistance and the weatherability of the aerated building block, and cooperate with the porous ceramsite, the boron slag and the blast furnace water quenching slag to improve the fire resistance and the heat insulation property of the aerated building block. The aerated building block made in the invention has the advantages of excellent comprehensive performances, excellent mechanical performances, excellent weatherability, excellent acid and alkali corrosion resistance, excellent ageing crack resistance, excellent heat insulation property and excellent fire resistance.
Firebrick dust-containing aerated building block and making method thereof
WU CHUANXING (Autor:in)
27.01.2016
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
Polyacrylonitrile pulp-containing aerated building block and making method thereof
Europäisches Patentamt | 2016
|Mould-proof aerated building block and making method thereof
Europäisches Patentamt | 2016
|Corrosion resistant aerated building block and making method thereof
Europäisches Patentamt | 2016
|