Novel building material and external wall construction method thereof
The invention relates to an environment-friendly soft ceramic tile and a construction method thereof. The construction method of the environment-friendly soft ceramic tile is composed of the followingsteps of (1) preparing a modifier; (2) preparing a composite sepiolite material; and (3) preparing a soft porcelain material, crushing the composite sepiolite material to 15000-20000, selecting a composite adsorbent with great adsorption area as the main material on the selection of the material, extremely strong adsorption effect on pollutants in the air, crushing and grinding the composite sepiolite material to 15000-20000 mesh, and enhancing the effect while the composite sepiolite material is provided with great adsorption surface area. By modifying the composite adsorbent, there is an excellent adsorption effect on the trace amount of harmful organic gas in the air due to the fact that the charge of a double-aminopropyl octahedral cage-type silsesquioxane is large.
本发明涉及一种环保型软瓷砖及其施工方法,由以下步骤组成:(1)改性剂的制备:(2)复合海泡石材料的制备;(3)软瓷材料的制备,并且将复合海泡石材料粉碎至15000‑20000,在材料的选择上选用了吸附面积极大的以海泡石为主的复合吸附剂,对空气中的污染物有极强的吸附效果,将复合海泡石材料破碎碾磨至15000‑20000目在其本身就有极大的吸附表面积的同时可以增强效果。通过对复合吸附剂的改性,由于双氨丙基八聚六面体笼型倍半硅氧烷所带的电荷较多,对空气中痕量的有害有机气体有优异的吸附作用。
Novel building material and external wall construction method thereof
The invention relates to an environment-friendly soft ceramic tile and a construction method thereof. The construction method of the environment-friendly soft ceramic tile is composed of the followingsteps of (1) preparing a modifier; (2) preparing a composite sepiolite material; and (3) preparing a soft porcelain material, crushing the composite sepiolite material to 15000-20000, selecting a composite adsorbent with great adsorption area as the main material on the selection of the material, extremely strong adsorption effect on pollutants in the air, crushing and grinding the composite sepiolite material to 15000-20000 mesh, and enhancing the effect while the composite sepiolite material is provided with great adsorption surface area. By modifying the composite adsorbent, there is an excellent adsorption effect on the trace amount of harmful organic gas in the air due to the fact that the charge of a double-aminopropyl octahedral cage-type silsesquioxane is large.
本发明涉及一种环保型软瓷砖及其施工方法,由以下步骤组成:(1)改性剂的制备:(2)复合海泡石材料的制备;(3)软瓷材料的制备,并且将复合海泡石材料粉碎至15000‑20000,在材料的选择上选用了吸附面积极大的以海泡石为主的复合吸附剂,对空气中的污染物有极强的吸附效果,将复合海泡石材料破碎碾磨至15000‑20000目在其本身就有极大的吸附表面积的同时可以增强效果。通过对复合吸附剂的改性,由于双氨丙基八聚六面体笼型倍半硅氧烷所带的电荷较多,对空气中痕量的有害有机气体有优异的吸附作用。
Novel building material and external wall construction method thereof
一种新型建材及其外墙施工方法
JIN WENJUAN (Autor:in) / XIONG WENDIAN (Autor:in) / JIN LIJUAN (Autor:in) / JIN LIUWO (Autor:in) / ZOU LIJUN (Autor:in) / XIE WENHONG (Autor:in) / XIONG WEIXING (Autor:in) / XIONG WENSHAN (Autor:in)
09.06.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
E04F
FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
,
Ausbau von Bauwerken, z.B. Treppen, Fußböden
/
C04B
Kalk
,
LIME
/
C07F
Acyclische, carbocyclische oder heterocyclische Verbindungen, die andere Elemente als Kohlenstoff, Wasserstoff, Halogen, Sauerstoff, Stickstoff, Schwefel, Selen oder Tellur enthalten
,
ACYCLIC, CARBOCYCLIC, OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM
Environment-friendly building external wall material and construction method thereof
Europäisches Patentamt | 2020
|Construction method of building external wall waterproof thermal insulation material
Europäisches Patentamt | 2022
|Novel pre-embedded building external scaffold wall connecting device and construction method thereof
Europäisches Patentamt | 2021
|Building external wall heat preservation system and construction method thereof
Europäisches Patentamt | 2020
|Fabricated building external wall insulation board and construction method thereof
Europäisches Patentamt | 2023
|