Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Aerated concrete dry-mixed plastering mortar and preparation method thereof
The invention discloses aerated concrete dry-mixed plastering mortar and a preparation method thereof. The aerated concrete dry-mixed plastering mortar comprises the following components in parts by weight: 250-350 parts of cement, 450-550 parts of machine-made fine sand, 650-750 parts of river sand, 1.2-1.8 parts of polypropylene fiber, 1-5 parts of a polycarboxylate superplasticizer, 5-10 partsof diatomite, 5-10 parts of silica fume, 5-10 parts of fly ash, 1-5 parts of starch ether and 10-15 parts of an admixture, wherein the admixture is prepared from the following components in parts by weight: 0.3 to 0.7 part of cellulose ether, 5 to 10 parts of sodium bentonite, 20 to 30 parts of glutinous rice flour, 10 to 15 parts of polyurethane sealant, 1 to 5 parts of graphene, 5 to 25 parts ofvermiculite powder and 10 to 40 parts of ethanol with a mass fraction of 90-93%. The aerated concrete dry-mixed plastering mortar disclosed by the invention has the advantages of high bonding strength, good workability, good water-retaining property and good crack resistance.
本发明公开了一种加气混凝土干混抹灰砂浆及其制备方法。加气混凝土干混抹灰砂浆包含以下重量份的组分:250‑350份水泥、450‑550份机制细砂、650‑750份河砂、1.2‑1.8份聚丙烯纤维、1‑5份聚羧酸减水剂、5‑10份硅藻土、5‑10份硅灰、5‑10份粉煤灰、1‑5份淀粉醚、10‑15份外加剂;外加剂包括以下重量份的组份:0.3‑0.7份纤维素醚、5‑10份钠基膨润土、20‑30份糯米粉、10‑15份聚氨酯密封胶、1‑5份石墨烯、5‑25份蛭石粉、10‑40份质量分数为90‑93%的乙醇。本发明的加气混凝土干混抹灰砂浆具有粘结强度高,和易性、保水性和抗裂性能好的优点。
Aerated concrete dry-mixed plastering mortar and preparation method thereof
The invention discloses aerated concrete dry-mixed plastering mortar and a preparation method thereof. The aerated concrete dry-mixed plastering mortar comprises the following components in parts by weight: 250-350 parts of cement, 450-550 parts of machine-made fine sand, 650-750 parts of river sand, 1.2-1.8 parts of polypropylene fiber, 1-5 parts of a polycarboxylate superplasticizer, 5-10 partsof diatomite, 5-10 parts of silica fume, 5-10 parts of fly ash, 1-5 parts of starch ether and 10-15 parts of an admixture, wherein the admixture is prepared from the following components in parts by weight: 0.3 to 0.7 part of cellulose ether, 5 to 10 parts of sodium bentonite, 20 to 30 parts of glutinous rice flour, 10 to 15 parts of polyurethane sealant, 1 to 5 parts of graphene, 5 to 25 parts ofvermiculite powder and 10 to 40 parts of ethanol with a mass fraction of 90-93%. The aerated concrete dry-mixed plastering mortar disclosed by the invention has the advantages of high bonding strength, good workability, good water-retaining property and good crack resistance.
本发明公开了一种加气混凝土干混抹灰砂浆及其制备方法。加气混凝土干混抹灰砂浆包含以下重量份的组分:250‑350份水泥、450‑550份机制细砂、650‑750份河砂、1.2‑1.8份聚丙烯纤维、1‑5份聚羧酸减水剂、5‑10份硅藻土、5‑10份硅灰、5‑10份粉煤灰、1‑5份淀粉醚、10‑15份外加剂;外加剂包括以下重量份的组份:0.3‑0.7份纤维素醚、5‑10份钠基膨润土、20‑30份糯米粉、10‑15份聚氨酯密封胶、1‑5份石墨烯、5‑25份蛭石粉、10‑40份质量分数为90‑93%的乙醇。本发明的加气混凝土干混抹灰砂浆具有粘结强度高,和易性、保水性和抗裂性能好的优点。
Aerated concrete dry-mixed plastering mortar and preparation method thereof
加气混凝土干混抹灰砂浆及其制备方法
WEI CHANGSHUN (Autor:in) / HAN GUOZHU (Autor:in) / ZHANG LIJUN (Autor:in)
19.06.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Aerated concrete dry-mixed plastering mortar and preparation method thereof
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2023
|Preparation method of waterproof plastering mortar and plastering mortar
Europäisches Patentamt | 2023
|Dry-mixed plastering mortar and preparation method thereof
Europäisches Patentamt | 2020
|Dry-mixed plastering mortar and preparation method thereof
Europäisches Patentamt | 2023
|