Method for manufacturing environment-friendly floor tile by replacing ceramic material with cementing material
The invention discloses a method for manufacturing an environment-friendly floor tile by replacing a ceramic material with a cementing material. The cementing material is prepared from the following raw materials: cement, a retarder, a water reducing agent, bentonite, granite powder, limestone, quartz sand and water. By limiting the composition of the cementing material, the strength and temperature resistance of the prepared environment-friendly floor tile are improved, the cementing material comprises granite stone powder and quartz sand, the strength of the environment-friendly floor tile can be improved, limestone is decomposed into powdery slaked lime after being calcined, and the powdery slaked lime can be used as an adhesive, so that stable combination of all the raw materials is guaranteed, and the strength of the environment-friendly floor tile is guaranteed.
利用胶凝材料替代陶瓷材料制作环保地砖的方法,胶凝材料由以下原料组成:水泥、缓凝剂、减水剂、皂土、花岗石粉、石灰石、石英砂、水,通过限定胶凝材料的组成,提高制备的环保地砖的强度和抗温性能,胶凝材料中包括花岗岩石粉和石英砂可提高环保地砖强度,石灰石经过煅烧后消解成粉状熟石灰,可作为粘合剂,保证各原料之间的稳定结合,保证环保地砖的强度。
Method for manufacturing environment-friendly floor tile by replacing ceramic material with cementing material
The invention discloses a method for manufacturing an environment-friendly floor tile by replacing a ceramic material with a cementing material. The cementing material is prepared from the following raw materials: cement, a retarder, a water reducing agent, bentonite, granite powder, limestone, quartz sand and water. By limiting the composition of the cementing material, the strength and temperature resistance of the prepared environment-friendly floor tile are improved, the cementing material comprises granite stone powder and quartz sand, the strength of the environment-friendly floor tile can be improved, limestone is decomposed into powdery slaked lime after being calcined, and the powdery slaked lime can be used as an adhesive, so that stable combination of all the raw materials is guaranteed, and the strength of the environment-friendly floor tile is guaranteed.
利用胶凝材料替代陶瓷材料制作环保地砖的方法,胶凝材料由以下原料组成:水泥、缓凝剂、减水剂、皂土、花岗石粉、石灰石、石英砂、水,通过限定胶凝材料的组成,提高制备的环保地砖的强度和抗温性能,胶凝材料中包括花岗岩石粉和石英砂可提高环保地砖强度,石灰石经过煅烧后消解成粉状熟石灰,可作为粘合剂,保证各原料之间的稳定结合,保证环保地砖的强度。
Method for manufacturing environment-friendly floor tile by replacing ceramic material with cementing material
利用胶凝材料替代陶瓷材料制作环保地砖的方法
HUANG FEIQIAO (Autor:in)
03.07.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2015
|Gypsum-based ceramic tile cementing material and preparation method thereof
Europäisches Patentamt | 2022
|Environment-friendly ceramic floor tile and preparation method thereof
Europäisches Patentamt | 2021
|Environment-friendly ceramic tile floor and paving method thereof
Europäisches Patentamt | 2023
|