Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Steel slag asphalt concrete formula
The invention provides a steel slag asphalt concrete formula. The steel slag asphalt concrete formula comprises the following components in percentage by weight: 28% of steel slag 0-3mm, 18% of steelslag 3-8mm, 24% of steel slag 8-16mm, 16% of steel slag 16-22mm, 14% of steel slag 22-32mm and 3.8% of asphalt oil. Steel slag raw materials with different specifications are used for replacing traditional stone materials; the stone exploitation and the use of non-renewable resources are reduced; the abundant steel slag raw materials are fully utilized, the steel slag raw materials with differentspecifications can replace stone, the fusion and filling of the mixture can be fully improved, the asphalt oil is mixed with the steel slag raw materials with different specifications, the supportingstrength of the concrete is effectively improved, and the pressure resistance of the concrete is improved.
本发明提供一种钢渣沥青混凝土配方。所述钢渣沥青混凝土配方按重量百分比:0‑3mm的钢渣28%,3‑8mm的钢渣18%,8‑16mm的钢渣24%,16‑22mm的钢渣16%,22‑32mm的钢渣14%,沥青油3.8%;所述0‑3mm的钢渣28%,3‑8mm的钢渣20%,8‑16mm的钢渣27%,16‑22mm的钢渣15%,22‑32mm的钢渣10%,沥青油4.2%。本发明提供的钢渣沥青混凝土配方具有通过采用不同规格的钢渣原料代替传统的石料,降低石料的开采和不可再生资源的使用,充分利用资源量大的钢渣原料,不同规格的钢渣原料代替石料可以充分的提高混合料的融合和填充,通过沥青油与不同规格的钢渣原料进行混合,有效的提高混凝土的支撑强度,提高混凝土的抗压能力。
Steel slag asphalt concrete formula
The invention provides a steel slag asphalt concrete formula. The steel slag asphalt concrete formula comprises the following components in percentage by weight: 28% of steel slag 0-3mm, 18% of steelslag 3-8mm, 24% of steel slag 8-16mm, 16% of steel slag 16-22mm, 14% of steel slag 22-32mm and 3.8% of asphalt oil. Steel slag raw materials with different specifications are used for replacing traditional stone materials; the stone exploitation and the use of non-renewable resources are reduced; the abundant steel slag raw materials are fully utilized, the steel slag raw materials with differentspecifications can replace stone, the fusion and filling of the mixture can be fully improved, the asphalt oil is mixed with the steel slag raw materials with different specifications, the supportingstrength of the concrete is effectively improved, and the pressure resistance of the concrete is improved.
本发明提供一种钢渣沥青混凝土配方。所述钢渣沥青混凝土配方按重量百分比:0‑3mm的钢渣28%,3‑8mm的钢渣18%,8‑16mm的钢渣24%,16‑22mm的钢渣16%,22‑32mm的钢渣14%,沥青油3.8%;所述0‑3mm的钢渣28%,3‑8mm的钢渣20%,8‑16mm的钢渣27%,16‑22mm的钢渣15%,22‑32mm的钢渣10%,沥青油4.2%。本发明提供的钢渣沥青混凝土配方具有通过采用不同规格的钢渣原料代替传统的石料,降低石料的开采和不可再生资源的使用,充分利用资源量大的钢渣原料,不同规格的钢渣原料代替石料可以充分的提高混合料的融合和填充,通过沥青油与不同规格的钢渣原料进行混合,有效的提高混凝土的支撑强度,提高混凝土的抗压能力。
Steel slag asphalt concrete formula
一种钢渣沥青混凝土配方
WANG JIAN (Autor:in) / WANG YINUO (Autor:in)
25.09.2020
Patent
Elektronische Ressource
Chinesisch
Europäisches Patentamt | 2021
|Steel slag asphalt concrete mix proportion design method
Europäisches Patentamt | 2022
|Steel slag asphalt concrete and preparation method thereof
Europäisches Patentamt | 2023
|