Soaking type trace element slow-release cup core and manufacturing method thereof
The invention relates to a soaking type trace element slow-release cup core and a manufacturing method thereof. The cup core is provided with a cavity and water permeable holes, and the cavity wall ofthe cavity is provided with a trace element filling layer and a nanoscale nutrition slow-release channel. Purple sand mud, diatom minerals, nano zinc dioxide, titanium oxide, magnesium oxide, Muyu stone, feldspar, medical stone, tourmaline, loess stone powder and kaolin are combined into a combination. Nanometer zinc dioxide, titanium oxide, magnesium oxide, Muyu stone and tourmaline are enabledto go deep into micron-sized pores of diatom minerals and medical stone; a material structure of purple sand mud, feldspar, loess stone powder and kaolin is firmly embedded on the surfaces of diatom minerals, medical stone, zinc dioxide, titanium oxide, magnesium oxide, Muyu stone and tourmaline, and the soaking type trace element slow-release cup core with a full-distributed micropore structure is fired. The slow-release cup core is placed in a tea cup to be soaked in tea water, brewing and taking are convenient, human health can be promoted, and the practical application value is achieved.
本发明涉及一种浸泡型微量元素缓释杯芯及其制作方法,杯芯设有腔体和透水孔,腔体腔壁设有微量元素填充层,并设有纳米级营养缓释通道。将紫砂泥、硅藻矿物、纳米二氧化锌、氧化钛、氧化镁、木鱼石、长钾石、麦饭石、碧玺、黄土石粉和高岭土原料结合成组合体,使纳米二氧化锌、氧化钛、氧化镁、木鱼石、碧玺深入到硅藻矿物和麦饭石的微米级多孔中去,利用紫砂泥、长钾石、黄土石粉和高岭土的材料结构牢牢地镶嵌在硅藻矿物、麦饭石、二氧化锌、氧化钛、氧化镁、木鱼石和碧玺的表面,烧制成具有满布微孔结构的浸泡型微量元素缓释杯芯。本发明的缓释杯芯放在茶水杯里浸泡茶水,泡服方便,可促进人体健康,具有实际应用价值。
Soaking type trace element slow-release cup core and manufacturing method thereof
The invention relates to a soaking type trace element slow-release cup core and a manufacturing method thereof. The cup core is provided with a cavity and water permeable holes, and the cavity wall ofthe cavity is provided with a trace element filling layer and a nanoscale nutrition slow-release channel. Purple sand mud, diatom minerals, nano zinc dioxide, titanium oxide, magnesium oxide, Muyu stone, feldspar, medical stone, tourmaline, loess stone powder and kaolin are combined into a combination. Nanometer zinc dioxide, titanium oxide, magnesium oxide, Muyu stone and tourmaline are enabledto go deep into micron-sized pores of diatom minerals and medical stone; a material structure of purple sand mud, feldspar, loess stone powder and kaolin is firmly embedded on the surfaces of diatom minerals, medical stone, zinc dioxide, titanium oxide, magnesium oxide, Muyu stone and tourmaline, and the soaking type trace element slow-release cup core with a full-distributed micropore structure is fired. The slow-release cup core is placed in a tea cup to be soaked in tea water, brewing and taking are convenient, human health can be promoted, and the practical application value is achieved.
本发明涉及一种浸泡型微量元素缓释杯芯及其制作方法,杯芯设有腔体和透水孔,腔体腔壁设有微量元素填充层,并设有纳米级营养缓释通道。将紫砂泥、硅藻矿物、纳米二氧化锌、氧化钛、氧化镁、木鱼石、长钾石、麦饭石、碧玺、黄土石粉和高岭土原料结合成组合体,使纳米二氧化锌、氧化钛、氧化镁、木鱼石、碧玺深入到硅藻矿物和麦饭石的微米级多孔中去,利用紫砂泥、长钾石、黄土石粉和高岭土的材料结构牢牢地镶嵌在硅藻矿物、麦饭石、二氧化锌、氧化钛、氧化镁、木鱼石和碧玺的表面,烧制成具有满布微孔结构的浸泡型微量元素缓释杯芯。本发明的缓释杯芯放在茶水杯里浸泡茶水,泡服方便,可促进人体健康,具有实际应用价值。
Soaking type trace element slow-release cup core and manufacturing method thereof
浸泡型微量元素缓释杯芯及其制作方法
ZHANG YONG (Autor:in) / ZHANG ZHILONG (Autor:in) / LI JIANGBO (Autor:in)
20.10.2020
Patent
Elektronische Ressource
Chinesisch
Trace element-containing slow-release cup and manufacturing method thereof
Europäisches Patentamt | 2020
|Manufacturing method of trace element slow-release pot
Europäisches Patentamt | 2021
|Rare earth-containing trace element slow-release cup and manufacturing method thereof
Europäisches Patentamt | 2020
|Manufacturing method of ceramic complex trace element slow-release pot
Europäisches Patentamt | 2021
|Manufacturing method of ceramic complex trace element slow-release pot
Europäisches Patentamt | 2021
|