Decorative building block containing glass slag and preparation method thereof
The invention discloses a decorative building block containing glass slag. The decorative building block is prepared from the following raw materials in parts by weight: 320 to 360 parts of glass slag, 320 to 360 parts of tailing slag, 300 to 350 parts of building solid waste, 160 to 200 parts of carbon fibers, 160 to 200 parts of polypropylene fibers, 125 to 165 parts of PVA fibers, 85 to 125 parts of graphene, 155 to 195 parts of semi-hydrated gypsum, 235 to 375 parts of cement, 65 to 105 parts of a water reducer, 85 to 95 parts of a foaming agent, and 55 to 95 parts of a foam stabilizer. The glass slag, the tailing slag and the building solid waste are used as raw materials for preparing the decorative building block, the production cost of the decorative building block is greatly reduced, the prepared decorative building block is good in durability, and the crack resistance of the decorative building block is enhanced; waste is turned into wealth, resources are utilized to the maximum extent, and energy conservation and environmental protection are achieved.
本发明公开了一种含有玻璃渣的装饰砌块,由以下重量份的原料制成:玻璃渣320~360份、尾矿渣320~360份、建筑固体废弃物300~350份、碳纤维160~200份、聚丙烯纤维160~200份、PVA纤维125~165份、石墨烯85~125份、半水石膏155~195份、水泥235~375份、减水剂65~105份、发泡剂85~125份、稳泡剂55~95份。本申请将玻璃渣、尾矿渣、建筑固体废弃物作为原料制备装饰砌块,大大降低了装饰砌块的生产成本,且制得的装饰砌块耐久性良好,装饰砌块的抗裂能力增强;变废为宝,将资源最大化利用,节能环保。
Decorative building block containing glass slag and preparation method thereof
The invention discloses a decorative building block containing glass slag. The decorative building block is prepared from the following raw materials in parts by weight: 320 to 360 parts of glass slag, 320 to 360 parts of tailing slag, 300 to 350 parts of building solid waste, 160 to 200 parts of carbon fibers, 160 to 200 parts of polypropylene fibers, 125 to 165 parts of PVA fibers, 85 to 125 parts of graphene, 155 to 195 parts of semi-hydrated gypsum, 235 to 375 parts of cement, 65 to 105 parts of a water reducer, 85 to 95 parts of a foaming agent, and 55 to 95 parts of a foam stabilizer. The glass slag, the tailing slag and the building solid waste are used as raw materials for preparing the decorative building block, the production cost of the decorative building block is greatly reduced, the prepared decorative building block is good in durability, and the crack resistance of the decorative building block is enhanced; waste is turned into wealth, resources are utilized to the maximum extent, and energy conservation and environmental protection are achieved.
本发明公开了一种含有玻璃渣的装饰砌块,由以下重量份的原料制成:玻璃渣320~360份、尾矿渣320~360份、建筑固体废弃物300~350份、碳纤维160~200份、聚丙烯纤维160~200份、PVA纤维125~165份、石墨烯85~125份、半水石膏155~195份、水泥235~375份、减水剂65~105份、发泡剂85~125份、稳泡剂55~95份。本申请将玻璃渣、尾矿渣、建筑固体废弃物作为原料制备装饰砌块,大大降低了装饰砌块的生产成本,且制得的装饰砌块耐久性良好,装饰砌块的抗裂能力增强;变废为宝,将资源最大化利用,节能环保。
Decorative building block containing glass slag and preparation method thereof
一种含有玻璃渣的装饰砌块及其制备方法
LI LIUYI (Autor:in) / ZHONG JIANQIANG (Autor:in) / LIU ZHIFU (Autor:in) / LI JIANWEI (Autor:in) / LIU AIJUN (Autor:in)
22.01.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Glass slag decorative brick and preparation method thereof
Europäisches Patentamt | 2021
|Mine slag-based aerated building block and preparation method thereof
Europäisches Patentamt | 2020
|Copper slag oxalate-based bare concrete decorative plate and preparation method thereof
Europäisches Patentamt | 2023
|Novel barium slag fly ash hollow building block and preparation method thereof
Europäisches Patentamt | 2020
|Copper slag concrete block and preparation method thereof
Europäisches Patentamt | 2022
|