The invention belongs to the technical field of concrete production, and particularly relates to a foamed concrete block and a production method thereof. The foamed concrete block is prepared from, byweight, 25-45 parts of waste stone slurry powder, 15-35 parts of cement, 15-35 parts of water, 1-1.5 parts of a chemical foaming agent and 0.1-0.5 part of an external additive; the product has the advantage of being low in production cost; the production method of the foamed concrete block comprises the following steps: S1, preparing raw materials, wherein the raw materials comprise the followingcomponents in parts by weight: 25-45 parts of waste stone slurry powder, 15-35 parts of cement, 15-35 parts of water, 1-1.5 parts of a chemical foaming agent and 0.1-0.5 part of an external additive;S2, screening stone slurry powder with qualified granularity; S3, mixing and stirring the raw materials to obtain concrete slurry; S4, pouring the concrete slurry into a mold for foaming; S5, demolding and taking out the concrete block semi-finished product, and placing the concrete block semi-finished product in a curing chamber for curing time t1; S6, cutting the concrete blocks according to specifications; and S7, the concrete blocks are placed in a curing chamber to be cured for the time t2. The production method has the advantages of simple process, energy conservation, environmental protection, high product quality and the like.
本发明属于混凝土生产技术领域,具体涉及一种发泡混凝土砌块及其生产方法,以重量份计算,发泡混凝土砌块包括废弃石浆粉25~45份,水泥15~35份,水15~35份,化学发泡剂1~1.5份,外添加剂0.1~0.5份,其具有生产成本低的优点;发泡混凝土砌块生产方法包括以下步骤:S1:预备原料,原料各组分的重量份为废弃石浆粉25~45份,水泥15~35份,水15~35份,化学发泡剂1~1.5份,外添加剂0.1~0.5份;S2:筛选粒度合格的石浆粉;S3:原料混合搅拌获得混凝土浆料;S4:将混凝土浆料倒入模具发泡;S5:将混凝土砌块半成品脱模取出,放置在养护室内养护时间t1;S6:按规格切割混凝土砌块;S7:将混凝土砌块放在养护室内养护时间t2。该生产方法具有流程简单、节能环保、制得产品质量高等优点。
The invention belongs to the technical field of concrete production, and particularly relates to a foamed concrete block and a production method thereof. The foamed concrete block is prepared from, byweight, 25-45 parts of waste stone slurry powder, 15-35 parts of cement, 15-35 parts of water, 1-1.5 parts of a chemical foaming agent and 0.1-0.5 part of an external additive; the product has the advantage of being low in production cost; the production method of the foamed concrete block comprises the following steps: S1, preparing raw materials, wherein the raw materials comprise the followingcomponents in parts by weight: 25-45 parts of waste stone slurry powder, 15-35 parts of cement, 15-35 parts of water, 1-1.5 parts of a chemical foaming agent and 0.1-0.5 part of an external additive;S2, screening stone slurry powder with qualified granularity; S3, mixing and stirring the raw materials to obtain concrete slurry; S4, pouring the concrete slurry into a mold for foaming; S5, demolding and taking out the concrete block semi-finished product, and placing the concrete block semi-finished product in a curing chamber for curing time t1; S6, cutting the concrete blocks according to specifications; and S7, the concrete blocks are placed in a curing chamber to be cured for the time t2. The production method has the advantages of simple process, energy conservation, environmental protection, high product quality and the like.
本发明属于混凝土生产技术领域,具体涉及一种发泡混凝土砌块及其生产方法,以重量份计算,发泡混凝土砌块包括废弃石浆粉25~45份,水泥15~35份,水15~35份,化学发泡剂1~1.5份,外添加剂0.1~0.5份,其具有生产成本低的优点;发泡混凝土砌块生产方法包括以下步骤:S1:预备原料,原料各组分的重量份为废弃石浆粉25~45份,水泥15~35份,水15~35份,化学发泡剂1~1.5份,外添加剂0.1~0.5份;S2:筛选粒度合格的石浆粉;S3:原料混合搅拌获得混凝土浆料;S4:将混凝土浆料倒入模具发泡;S5:将混凝土砌块半成品脱模取出,放置在养护室内养护时间t1;S6:按规格切割混凝土砌块;S7:将混凝土砌块放在养护室内养护时间t2。该生产方法具有流程简单、节能环保、制得产品质量高等优点。
Core foamed concrete thermal insulation building block and production process thereof
Europäisches Patentamt | 2024
|Lightweight foamed thermal insulation concrete block and preparation method thereof
Europäisches Patentamt | 2020
|Manufacturing Method of Waterproof Foamed Concrete Block
Europäisches Patentamt | 2019
Manufacturing Method of Waterproof Foamed Concrete Block
Europäisches Patentamt | 2019
|