The invention discloses non-slip glaze and a processing method of a non-slip glazed brick, and relates to the field of non-slip glazed brick processing, the non-slip glaze comprises the following components by weight: 30-40 parts of frit particles, 20-30 parts of aluminum oxide, 15-20 parts of diatomite, 15-20 parts of shell powder, 0.2-0.3 part of carbon nanotubes and 5-10 parts of an additive; and each part of frit particles comprises 0.5-0.6 part of silicon dioxide, 0.1-0.2 part of zinc oxide, 0.1-0.2 part of magnesium oxide, 0.05-0.1 part of calcium oxide and 0.01-0.02 part of ferric oxide. According to the non-slip glaze, the friction coefficient of the ground is greatly increased by utilizing atmospheric pressure, the non-slip purpose is achieved, and in addition, the non-slip glaze also has the effects of wear resistance, fire prevention, corrosion prevention and pollution resistance; and the processing method of the anti-slip glazed brick is simple to operate, and the prepared anti-slip glazed brick has good anti-pollution and anti-slip properties, and is flat and beautiful.
一种止滑釉及止滑釉砖的加工方法,涉及止滑釉砖加工领域,止滑釉按照重量配比,其组成成分包括30‑40份的熔块粒、20‑30份的三氧化二铝、15‑20份的硅藻土、15‑20份的贝壳粉、0.2‑0.3份的纳米碳管和5‑10份的添加剂;每份熔块粒包括0.5‑0.6份的二氧化硅、0.1‑0.2份的氧化锌、0.1‑0.2份的氧化镁、0.05‑0.1份的氧化钙和0.01‑0.02份的三氧化二铁。本发明中的止滑釉利用大气压力,使地面摩擦系数大大增加,实现防滑的目的,此外还具有耐磨、防火、防腐蚀和抗污的效果;止滑釉砖的加工方法操作简单,制备的到的止滑釉砖抗污、防滑性好,平整美观。
The invention discloses non-slip glaze and a processing method of a non-slip glazed brick, and relates to the field of non-slip glazed brick processing, the non-slip glaze comprises the following components by weight: 30-40 parts of frit particles, 20-30 parts of aluminum oxide, 15-20 parts of diatomite, 15-20 parts of shell powder, 0.2-0.3 part of carbon nanotubes and 5-10 parts of an additive; and each part of frit particles comprises 0.5-0.6 part of silicon dioxide, 0.1-0.2 part of zinc oxide, 0.1-0.2 part of magnesium oxide, 0.05-0.1 part of calcium oxide and 0.01-0.02 part of ferric oxide. According to the non-slip glaze, the friction coefficient of the ground is greatly increased by utilizing atmospheric pressure, the non-slip purpose is achieved, and in addition, the non-slip glaze also has the effects of wear resistance, fire prevention, corrosion prevention and pollution resistance; and the processing method of the anti-slip glazed brick is simple to operate, and the prepared anti-slip glazed brick has good anti-pollution and anti-slip properties, and is flat and beautiful.
一种止滑釉及止滑釉砖的加工方法,涉及止滑釉砖加工领域,止滑釉按照重量配比,其组成成分包括30‑40份的熔块粒、20‑30份的三氧化二铝、15‑20份的硅藻土、15‑20份的贝壳粉、0.2‑0.3份的纳米碳管和5‑10份的添加剂;每份熔块粒包括0.5‑0.6份的二氧化硅、0.1‑0.2份的氧化锌、0.1‑0.2份的氧化镁、0.05‑0.1份的氧化钙和0.01‑0.02份的三氧化二铁。本发明中的止滑釉利用大气压力,使地面摩擦系数大大增加,实现防滑的目的,此外还具有耐磨、防火、防腐蚀和抗污的效果;止滑釉砖的加工方法操作简单,制备的到的止滑釉砖抗污、防滑性好,平整美观。
Non-slip glaze and processing method of non-slip glazed brick
一种止滑釉及止滑釉砖的加工方法
HU YAO (Autor:in)
11.06.2021
Patent
Elektronische Ressource
Chinesisch
Glaze, non-slip brick with dry-grain-imitating effect and preparation method of non-slip brick
Europäisches Patentamt | 2023
|Europäisches Patentamt | 2015
|Wear-resistant antifouling glazed brick glaze and preparation method thereof
Europäisches Patentamt | 2020
|BRICK SLIP, METHOD OF MANUFACTURING A BRICK SLIP, AND BRICK SLIP ASSEMBLY
Europäisches Patentamt | 2023
|Brick slip, method of manufacturing a brick slip, and brick slip assembly
Europäisches Patentamt | 2023
|