Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Formula for light wallboard and production process for light wallboard
The invention discloses a formula and a production process for a light wallboard. The production process comprises the steps that 3) forming treatment is carried out, specifically, a mixed material in the step 2) is firstly introduced into a mold in a light wallboard forming machine for pouring, then the mold is continuously vibrated and knocked by a stainless steel pipe, supplement operation is carried out along with the vibration and knocking of the stainless steel pipe, then a roller shaft rolls back and forth on the surface of the mold, and finally, the light wallboard forming machine is started; 4) curing treatment is carried out, specifically, the light wallboard prepared in the step 3) is taken out through stripping, then is placed in a closed shade for curing operation, the temperature is controlled to be between 10 and 15 DEG C, the curing time is controlled to be between 10 and 12 hours, and direct sunlight needs to be avoided at the same time; and (5) maintenance treatment is carried out, specifically, the light wallboard in the step (4) is put into a steam chamber for maintenance operation, the temperature of introduced steam is controlled to be 70-80 DEG C, the maintenance time is controlled to be 3-4 hours, and then the light wallboard is naturally cooled to the normal temperature. The formula has the characteristics of being high in practicability and high in production efficiency.
本发明公开了一种轻质墙板配方及生产工艺,3)成型处理:先将步骤2)中的混料导入轻质墙板成型机中的模具内进行浇注,再用不锈钢管不断对模具进行振动敲打,并随之进行补料操作,之后用辊轴在模具表面来回滚动,最后开启轻质墙板成型机;4)固化处理:先将步骤3)中所制得的轻质墙板经脱模取出后,再放入密闭的阴凉处进行固化操作,并控制温度在10至15度,且固化时间控制在10至12小时,同时需避免阳光直射;5)养护处理:先将步骤4)中的轻质墙板放入蒸汽室内进行养护操作,且通入的蒸汽温度控制在70至80度,养护时间控制在3至4小时,之后将轻质墙板自然冷却至常温即可;本发明,具有实用性强和生产效率高的特点。
Formula for light wallboard and production process for light wallboard
The invention discloses a formula and a production process for a light wallboard. The production process comprises the steps that 3) forming treatment is carried out, specifically, a mixed material in the step 2) is firstly introduced into a mold in a light wallboard forming machine for pouring, then the mold is continuously vibrated and knocked by a stainless steel pipe, supplement operation is carried out along with the vibration and knocking of the stainless steel pipe, then a roller shaft rolls back and forth on the surface of the mold, and finally, the light wallboard forming machine is started; 4) curing treatment is carried out, specifically, the light wallboard prepared in the step 3) is taken out through stripping, then is placed in a closed shade for curing operation, the temperature is controlled to be between 10 and 15 DEG C, the curing time is controlled to be between 10 and 12 hours, and direct sunlight needs to be avoided at the same time; and (5) maintenance treatment is carried out, specifically, the light wallboard in the step (4) is put into a steam chamber for maintenance operation, the temperature of introduced steam is controlled to be 70-80 DEG C, the maintenance time is controlled to be 3-4 hours, and then the light wallboard is naturally cooled to the normal temperature. The formula has the characteristics of being high in practicability and high in production efficiency.
本发明公开了一种轻质墙板配方及生产工艺,3)成型处理:先将步骤2)中的混料导入轻质墙板成型机中的模具内进行浇注,再用不锈钢管不断对模具进行振动敲打,并随之进行补料操作,之后用辊轴在模具表面来回滚动,最后开启轻质墙板成型机;4)固化处理:先将步骤3)中所制得的轻质墙板经脱模取出后,再放入密闭的阴凉处进行固化操作,并控制温度在10至15度,且固化时间控制在10至12小时,同时需避免阳光直射;5)养护处理:先将步骤4)中的轻质墙板放入蒸汽室内进行养护操作,且通入的蒸汽温度控制在70至80度,养护时间控制在3至4小时,之后将轻质墙板自然冷却至常温即可;本发明,具有实用性强和生产效率高的特点。
Formula for light wallboard and production process for light wallboard
一种轻质墙板配方及轻质墙板生产工艺
XIAO RENDE (Autor:in)
18.06.2021
Patent
Elektronische Ressource
Chinesisch
Light wallboard based on engineering residue soil and preparation process of light wallboard
Europäisches Patentamt | 2021
|Fabricated wallboard, continuous fabricated wallboard and continuous production process
Europäisches Patentamt | 2021
|