Easily-bonded porcelain tile green body for paving, porcelain tile comprising green body and preparation method of porcelain tile
The invention discloses a easily-bonded porcelain tile green body for paving, a porcelain tile comprising the green body and a preparation method of the porcelain tile green body. The easily-bonded porcelain tile blank body for paving comprises a low-shrinkage powder layer and an easily-bonded powder layer located on the bottom surface of the low-shrinkage powder layer; wherein the easily-bonded powder is prepared from the following raw materials in percentage by mass: 0.5-1.5% of manganese dioxide, 16-32% of an organic material and 66.0-83.5% of low-shrinkage powder; the low-shrinkage powder material is prepared from the following chemical components in percentage by mass: 60.0-68.0 percent of SiO2, 18.0-24.0 percent of Al2O3, 1.5-5.0 percent of CaO, 0.51.5 percent of MgO, 2.5-3.5 percent of K2O and 1.5-2.5 percent of Na2O. According to the easily-bonded ceramic tile green body for paving, the bonding performance of the ceramic tile during paving can be greatly improved.
本发明公开一种铺贴易粘结的瓷质砖坯体、包含该坯体的瓷质砖及制备方法。所述铺贴易粘结的瓷质砖坯体包括低收缩粉料层和位于所述低收缩粉料层底面的易粘结粉料层;其中,易粘结粉料的原料组成包括:以质量百分比计,二氧化锰:0.5~1.5%,有机材料:16~32%,低收缩粉料:66.0~83.5%;所述低收缩粉料的化学组成包括:以质量百分比计,SiO2:60.0~68.0%、Al2O3:18.0~24.0%、CaO:1.5~5.0%、MgO:0.5~1.5%、K2O:2.5~3.5%、Na2O:1.5~2.5%。所述铺贴易粘结的瓷质砖坯体可大幅度提升瓷质砖铺贴时的粘结性能。
Easily-bonded porcelain tile green body for paving, porcelain tile comprising green body and preparation method of porcelain tile
The invention discloses a easily-bonded porcelain tile green body for paving, a porcelain tile comprising the green body and a preparation method of the porcelain tile green body. The easily-bonded porcelain tile blank body for paving comprises a low-shrinkage powder layer and an easily-bonded powder layer located on the bottom surface of the low-shrinkage powder layer; wherein the easily-bonded powder is prepared from the following raw materials in percentage by mass: 0.5-1.5% of manganese dioxide, 16-32% of an organic material and 66.0-83.5% of low-shrinkage powder; the low-shrinkage powder material is prepared from the following chemical components in percentage by mass: 60.0-68.0 percent of SiO2, 18.0-24.0 percent of Al2O3, 1.5-5.0 percent of CaO, 0.51.5 percent of MgO, 2.5-3.5 percent of K2O and 1.5-2.5 percent of Na2O. According to the easily-bonded ceramic tile green body for paving, the bonding performance of the ceramic tile during paving can be greatly improved.
本发明公开一种铺贴易粘结的瓷质砖坯体、包含该坯体的瓷质砖及制备方法。所述铺贴易粘结的瓷质砖坯体包括低收缩粉料层和位于所述低收缩粉料层底面的易粘结粉料层;其中,易粘结粉料的原料组成包括:以质量百分比计,二氧化锰:0.5~1.5%,有机材料:16~32%,低收缩粉料:66.0~83.5%;所述低收缩粉料的化学组成包括:以质量百分比计,SiO2:60.0~68.0%、Al2O3:18.0~24.0%、CaO:1.5~5.0%、MgO:0.5~1.5%、K2O:2.5~3.5%、Na2O:1.5~2.5%。所述铺贴易粘结的瓷质砖坯体可大幅度提升瓷质砖铺贴时的粘结性能。
Easily-bonded porcelain tile green body for paving, porcelain tile comprising green body and preparation method of porcelain tile
铺贴易粘结的瓷质砖坯体、包含该坯体的瓷质砖及制备方法
PAN LIMIN (Autor:in) / WANG LONGJUN (Autor:in) / WANG XIANCHAO (Autor:in) / CHENG KEMU (Autor:in) / XIE FANFENG (Autor:in)
18.06.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Low-shrinkage porcelain tile blank and porcelain tile prepared from same
Europäisches Patentamt | 2022
|