Lightweight energy-saving environment-friendly thermal insulation material and preparation method thereof
The invention discloses a lightweight energy-saving environment-friendly thermal insulation material which comprises the following components in parts by weight: 11-15 parts of polyurethane foam plastic, 6-10 parts of polypropylene fibers, 4-8 parts of waste asbestos, 5-9 parts of calcium carbonate powder, 3-7 parts of foam glass, 4-8 parts of Portland cement, 1-2 parts of an anti-cracking agent, 1-3 parts of an antioxidant, 3-7 parts of a cross-linking agent, 1-2 parts of a water reducing agent and 45-65 parts of water. The invention also provides a preparation method of the lightweight energy-saving environment-friendly thermal insulation material. Through the calcium carbonate powder and the Portland cement, the hardness of the thermal insulation material is improved after the calcium carbonate powder and the Portland cement are dissolved and cured with water; the thermal insulation material is not prone to cracking in the mounting and fixing process, and meanwhile the thermal insulation effect of the material is greatly improved by adding the polyurethane foam plastic, the polypropylene fibers and the waste asbestos.
本发明公开了一种轻质节能环保保温材料,其重量按下列配比:11‑15份聚氨酯泡沫塑料、6‑10份聚丙烯纤维、4‑8份废弃石棉、5‑9份碳酸钙粉、3‑7份泡沫玻璃、4‑8份硅酸盐水泥、1‑2份抗裂剂、1‑3份抗氧剂、3‑7份交联剂、1‑2份减水剂、45‑65份水。本发明还提供了一种轻质节能环保保温材料的制备方法。本发明通过碳酸钙粉与硅酸盐水泥,碳酸钙粉与硅酸盐水泥与水溶合固化后,提高了保温材料的硬度,在保温材料安装固定过程中不易发生开裂,同时加入聚氨酯泡沫塑料、聚丙烯纤维与废弃石棉,极大的提高了材料的保温效果。
Lightweight energy-saving environment-friendly thermal insulation material and preparation method thereof
The invention discloses a lightweight energy-saving environment-friendly thermal insulation material which comprises the following components in parts by weight: 11-15 parts of polyurethane foam plastic, 6-10 parts of polypropylene fibers, 4-8 parts of waste asbestos, 5-9 parts of calcium carbonate powder, 3-7 parts of foam glass, 4-8 parts of Portland cement, 1-2 parts of an anti-cracking agent, 1-3 parts of an antioxidant, 3-7 parts of a cross-linking agent, 1-2 parts of a water reducing agent and 45-65 parts of water. The invention also provides a preparation method of the lightweight energy-saving environment-friendly thermal insulation material. Through the calcium carbonate powder and the Portland cement, the hardness of the thermal insulation material is improved after the calcium carbonate powder and the Portland cement are dissolved and cured with water; the thermal insulation material is not prone to cracking in the mounting and fixing process, and meanwhile the thermal insulation effect of the material is greatly improved by adding the polyurethane foam plastic, the polypropylene fibers and the waste asbestos.
本发明公开了一种轻质节能环保保温材料,其重量按下列配比:11‑15份聚氨酯泡沫塑料、6‑10份聚丙烯纤维、4‑8份废弃石棉、5‑9份碳酸钙粉、3‑7份泡沫玻璃、4‑8份硅酸盐水泥、1‑2份抗裂剂、1‑3份抗氧剂、3‑7份交联剂、1‑2份减水剂、45‑65份水。本发明还提供了一种轻质节能环保保温材料的制备方法。本发明通过碳酸钙粉与硅酸盐水泥,碳酸钙粉与硅酸盐水泥与水溶合固化后,提高了保温材料的硬度,在保温材料安装固定过程中不易发生开裂,同时加入聚氨酯泡沫塑料、聚丙烯纤维与废弃石棉,极大的提高了材料的保温效果。
Lightweight energy-saving environment-friendly thermal insulation material and preparation method thereof
一种轻质节能环保保温材料及其制备方法
QI XI (Autor:in) / ZHANG CHONG (Autor:in) / CUI LEI (Autor:in) / YANG HUI (Autor:in)
29.06.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2021
|Environment-friendly energy-saving thermal insulation material
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2023
|Europäisches Patentamt | 2022
|Lightweight thermal-insulation environment-friendly concrete and preparation method thereof
Europäisches Patentamt | 2020
|