Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Method for preparing environment-friendly brick from fly ash of garbage power plant
The invention discloses a method for preparing an environment-friendly brick by utilizing fly ash of a garbage power plant, which belongs to the technical field of building environmental protection and comprises the following steps: (1) mixing materials and (2) compression molding. According to the method for preparing the environment-friendly brick from the fly ash of the garbage power plant, the fly ash, the cement, a stabilizer and the superfine clay are jointly mixed, the environment-friendly brick is prepared in a high-pressure forming mode, it is guaranteed that harmful ingredients in the fly ash are not prone to seepage out under the combined action of high pressure, the stabilizer and the superfine clay, the green and stability of the environment-friendly bricks are improved,the compressive strength of the finally prepared environment-friendly brick is not less than 60 MPa, and the environment-friendly brick is green and safe.
本发明公开了一种利用垃圾发电厂飞灰制备环保砖的方法,属于建筑环保技术领域,包括如下步骤:(1)混料处理、(2)压制成型。本发明提供了一种利用垃圾发电厂飞灰制备环保砖的方法,本方法是利用飞灰、水泥、稳定剂和超细粘土共同混合,采用高压成型的方式来制备环保砖,其中利用高压及稳定剂和超细粘土的共同作用,保证了飞灰中的有害成分不易外渗,提升了环保砖的绿色、稳定性,最终制得的环保砖抗压强度不小于60MPa,且绿色安全。
Method for preparing environment-friendly brick from fly ash of garbage power plant
The invention discloses a method for preparing an environment-friendly brick by utilizing fly ash of a garbage power plant, which belongs to the technical field of building environmental protection and comprises the following steps: (1) mixing materials and (2) compression molding. According to the method for preparing the environment-friendly brick from the fly ash of the garbage power plant, the fly ash, the cement, a stabilizer and the superfine clay are jointly mixed, the environment-friendly brick is prepared in a high-pressure forming mode, it is guaranteed that harmful ingredients in the fly ash are not prone to seepage out under the combined action of high pressure, the stabilizer and the superfine clay, the green and stability of the environment-friendly bricks are improved,the compressive strength of the finally prepared environment-friendly brick is not less than 60 MPa, and the environment-friendly brick is green and safe.
本发明公开了一种利用垃圾发电厂飞灰制备环保砖的方法,属于建筑环保技术领域,包括如下步骤:(1)混料处理、(2)压制成型。本发明提供了一种利用垃圾发电厂飞灰制备环保砖的方法,本方法是利用飞灰、水泥、稳定剂和超细粘土共同混合,采用高压成型的方式来制备环保砖,其中利用高压及稳定剂和超细粘土的共同作用,保证了飞灰中的有害成分不易外渗,提升了环保砖的绿色、稳定性,最终制得的环保砖抗压强度不小于60MPa,且绿色安全。
Method for preparing environment-friendly brick from fly ash of garbage power plant
一种利用垃圾发电厂飞灰制备环保砖的方法
LI QUANSHENG (Autor:in)
29.10.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Novel process for preparing environment-friendly brick from industrial waste slag garbage
Europäisches Patentamt | 2021
|Method for preparing granite slurry environment-friendly brick
Europäisches Patentamt | 2015
|Europäisches Patentamt | 2022
|