Sludge baking-free brick and preparation method thereof
The invention relates to a sludge baking-free brick and a preparation method thereof, and belongs to the technical field of building materials, the sludge baking-free brick is prepared from the following raw materials by weight: 1000-3000 parts of sludge, 100-500 parts of cement, 1-5 parts of a curing agent, 0-1000 parts of gravel, and 100-500 parts of water. The preparation method comprises the following steps: weighing the raw materials according to the ratio, uniformly stirring the raw materials in a stirrer, filling the mixture into a mold, compacting the mixture by using a compactor, and demolding to complete the preparation of the baking-free brick. According to the sludge baking-free brick and the preparation method thereof, waste is turned into wealth, the sludge and mineral substances contained in the sludge are fully utilized, the prepared sludge baking-free brick has high compressive strength and excellent performance, and the preparation method of the sludge baking-free brick is simple, convenient and easy to implement, low in cost and capable of achieving industrialized production.
本发明涉及的一种淤泥免烧砖及其制备方法,属于建筑材料技术领域,该免烧砖按照重量份计,由以下原料制备而成:淤泥:1000~3000份,水泥:100~500份,固化剂:1~5份,碎石:0~1000份,水:100~500份。将上述原料按照上述配比称量后在搅拌机中搅拌均匀,然后将上述混合料装入模具中,利用压实仪压实,经脱模后完成免烧砖制备。本发明变废为宝,充分利用了淤泥及其所含的矿物质,制得的淤泥免烧砖具有较高的抗压强度,性能优良,且该淤泥免烧砖的制备方法简便易行,成本较低,可工厂化生产。
Sludge baking-free brick and preparation method thereof
The invention relates to a sludge baking-free brick and a preparation method thereof, and belongs to the technical field of building materials, the sludge baking-free brick is prepared from the following raw materials by weight: 1000-3000 parts of sludge, 100-500 parts of cement, 1-5 parts of a curing agent, 0-1000 parts of gravel, and 100-500 parts of water. The preparation method comprises the following steps: weighing the raw materials according to the ratio, uniformly stirring the raw materials in a stirrer, filling the mixture into a mold, compacting the mixture by using a compactor, and demolding to complete the preparation of the baking-free brick. According to the sludge baking-free brick and the preparation method thereof, waste is turned into wealth, the sludge and mineral substances contained in the sludge are fully utilized, the prepared sludge baking-free brick has high compressive strength and excellent performance, and the preparation method of the sludge baking-free brick is simple, convenient and easy to implement, low in cost and capable of achieving industrialized production.
本发明涉及的一种淤泥免烧砖及其制备方法,属于建筑材料技术领域,该免烧砖按照重量份计,由以下原料制备而成:淤泥:1000~3000份,水泥:100~500份,固化剂:1~5份,碎石:0~1000份,水:100~500份。将上述原料按照上述配比称量后在搅拌机中搅拌均匀,然后将上述混合料装入模具中,利用压实仪压实,经脱模后完成免烧砖制备。本发明变废为宝,充分利用了淤泥及其所含的矿物质,制得的淤泥免烧砖具有较高的抗压强度,性能优良,且该淤泥免烧砖的制备方法简便易行,成本较低,可工厂化生产。
Sludge baking-free brick and preparation method thereof
一种淤泥免烧砖及其制备方法
YU ZHENGBAO (Autor:in) / WANG LEI (Autor:in) / KONG XUEFENG (Autor:in) / XU GUOXIN (Autor:in) / CHEN YONGZHOU (Autor:in) / FEI JIDONG (Autor:in) / SONG LIANPING (Autor:in) / LIU RUICHAO (Autor:in)
25.03.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Sludge-based baking-free brick and preparation method thereof
Europäisches Patentamt | 2024
|Iron tailing sludge baking-free brick and preparation method thereof
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2023
|High-water-content sludge baking-free brick and preparation method thereof
Europäisches Patentamt | 2022
|Sand washing sludge baking-free brick and preparation process thereof
Europäisches Patentamt | 2023
|