Preparation of capillary crystalline waterproof agent
The invention belongs to the technical field of waterproof agents, and particularly relates to a capillary crystalline waterproof agent and a preparation method thereof. The capillary crystalline waterproofing agent comprises the following important components: a complexing substance LA and complexing assistants MD and NE. The preparation method comprises the following steps: taking important components of a complexing substance LA: 30% of sodium methylsilanolate and 68% of poly-metal silicic acid; the complexing aid MD comprises the following important components: 0.3% of low-temperature activated aluminum oxide (gamma type) and styrene 18 *; the complexing auxiliary agent NE comprises the following important components: 1.7% of a surfactant and 2% of itaconic acid; the preparation of the solvent comprises the following steps: mixing the selected materials in proportion, pouring into a container, uniformly stirring, and standing for 5-7 minutes to obtain the solvent.
本发明属于防水剂技术领域,具体为一种渗透结晶型防水剂及其制备方法;所述的渗透结晶防水剂的重要组成部分为:络合物质LA,络合助剂MD、NE三种物质组成。制备方法如下:络合物质LA重要组成部分:甲基硅醇纳30%、聚多金属硅酸68%;络合助剂MD重要组成部分:低温活性氧化铝(伽玛型)0.3%、苯乙烯18*;络合助剂NE重要组成部分:表面活性剂1.7%、衣康酸2%;上述溶剂的调配,是将选好的材质按比例调配好倒入容器中搅拌均匀后,静置5‑7分钟后即可使用。
Preparation of capillary crystalline waterproof agent
The invention belongs to the technical field of waterproof agents, and particularly relates to a capillary crystalline waterproof agent and a preparation method thereof. The capillary crystalline waterproofing agent comprises the following important components: a complexing substance LA and complexing assistants MD and NE. The preparation method comprises the following steps: taking important components of a complexing substance LA: 30% of sodium methylsilanolate and 68% of poly-metal silicic acid; the complexing aid MD comprises the following important components: 0.3% of low-temperature activated aluminum oxide (gamma type) and styrene 18 *; the complexing auxiliary agent NE comprises the following important components: 1.7% of a surfactant and 2% of itaconic acid; the preparation of the solvent comprises the following steps: mixing the selected materials in proportion, pouring into a container, uniformly stirring, and standing for 5-7 minutes to obtain the solvent.
本发明属于防水剂技术领域,具体为一种渗透结晶型防水剂及其制备方法;所述的渗透结晶防水剂的重要组成部分为:络合物质LA,络合助剂MD、NE三种物质组成。制备方法如下:络合物质LA重要组成部分:甲基硅醇纳30%、聚多金属硅酸68%;络合助剂MD重要组成部分:低温活性氧化铝(伽玛型)0.3%、苯乙烯18*;络合助剂NE重要组成部分:表面活性剂1.7%、衣康酸2%;上述溶剂的调配,是将选好的材质按比例调配好倒入容器中搅拌均匀后,静置5‑7分钟后即可使用。
Preparation of capillary crystalline waterproof agent
一种渗透结晶防水剂的制备
ZHANG YUWEI (Autor:in)
19.04.2022
Patent
Elektronische Ressource
Chinesisch
Cement-based capillary crystalline waterproof agent and waterproof material
Europäisches Patentamt | 2024
|Water-based capillary crystalline waterproof agent and preparation method thereof
Europäisches Patentamt | 2022
|Europäisches Patentamt | 2023
|Capillary crystalline waterproof agent and production process thereof
Europäisches Patentamt | 2023
|Water-based capillary crystalline inorganic waterproof agent and preparation equipment thereof
Europäisches Patentamt | 2024
|