Technological method for firing Jianshui purple pottery
The invention discloses a process method for firing Jianshui purple pottery, which sequentially comprises the following steps: S1, material preparation: burning grass and trees, then loading the burnt plant ash into a container, oxidizing and burning to 1000 DEG C in a high-temperature kiln, taking out for later use after cooling, and collecting waste tea water for drinking tea at ordinary times for later use for glaze preparation; the preparation method comprises the following steps: mixing 76-80% of prepared plant ash, 19-20% of sodium carbonate with the purity of 99.9% and 0.05-0.06% of naturally dried Jianshui purple pottery clay, adding 3.8-4 times of strong tea water for dilution, continuously grinding in a porcelain glaze ball mill until the fineness is more than 300 meshes, taking out for later use, molding and drying to obtain a Jianshui purple pottery blank; according to the invention, works with different colors can be fired according to different reduction strengths; the operability is high, and the color texture layers are rich; the eating is safe; the natural flavor of the tea leaves can be protected in an original taste and flavor manner, and the original conversion effect of the Jianshui purple pottery on the tea leaves is not lost.
本发明公开了一种烧制建水紫陶的工艺方法,依次包括如下步骤:S1、备料:将草木燃烧后,再将燃烧过的草木灰装在容器内高温窑炉内氧化烧至1000℃,待冷却后取出备用,平时喝茶的废茶叶水收集备用釉料配制;取76‑80%的已备制好的草木灰,19‑20%的纯度为99.9%的碳酸钠,0.05‑0.06%的自然干燥后的建水紫陶泥,进行混合配兑,再加3.8‑4倍的浓茶水稀释后置于瓷质釉料球磨机里持续研磨至300目以上的细度取出备用,成型干燥成建水紫陶陶坯;本发明,根据不同的还原强度,可烧制出不同呈色的作品;可操作性大,色彩肌理层次丰富;食用安全;更环保,能原汁原味的保护好茶叶的自然风味,也不失建水紫陶原有的对茶叶的转化效果。
Technological method for firing Jianshui purple pottery
The invention discloses a process method for firing Jianshui purple pottery, which sequentially comprises the following steps: S1, material preparation: burning grass and trees, then loading the burnt plant ash into a container, oxidizing and burning to 1000 DEG C in a high-temperature kiln, taking out for later use after cooling, and collecting waste tea water for drinking tea at ordinary times for later use for glaze preparation; the preparation method comprises the following steps: mixing 76-80% of prepared plant ash, 19-20% of sodium carbonate with the purity of 99.9% and 0.05-0.06% of naturally dried Jianshui purple pottery clay, adding 3.8-4 times of strong tea water for dilution, continuously grinding in a porcelain glaze ball mill until the fineness is more than 300 meshes, taking out for later use, molding and drying to obtain a Jianshui purple pottery blank; according to the invention, works with different colors can be fired according to different reduction strengths; the operability is high, and the color texture layers are rich; the eating is safe; the natural flavor of the tea leaves can be protected in an original taste and flavor manner, and the original conversion effect of the Jianshui purple pottery on the tea leaves is not lost.
本发明公开了一种烧制建水紫陶的工艺方法,依次包括如下步骤:S1、备料:将草木燃烧后,再将燃烧过的草木灰装在容器内高温窑炉内氧化烧至1000℃,待冷却后取出备用,平时喝茶的废茶叶水收集备用釉料配制;取76‑80%的已备制好的草木灰,19‑20%的纯度为99.9%的碳酸钠,0.05‑0.06%的自然干燥后的建水紫陶泥,进行混合配兑,再加3.8‑4倍的浓茶水稀释后置于瓷质釉料球磨机里持续研磨至300目以上的细度取出备用,成型干燥成建水紫陶陶坯;本发明,根据不同的还原强度,可烧制出不同呈色的作品;可操作性大,色彩肌理层次丰富;食用安全;更环保,能原汁原味的保护好茶叶的自然风味,也不失建水紫陶原有的对茶叶的转化效果。
Technological method for firing Jianshui purple pottery
一种烧制建水紫陶的工艺方法
YANG XUEHUI (Autor:in)
10.06.2022
Patent
Elektronische Ressource
Chinesisch
Firewood firing method capable of firing Jianshui purple pottery with jade effect
Europäisches Patentamt | 2024
|Jianshui pottery firewood-fired pug formula and firing process
Europäisches Patentamt | 2023
|Formula for firing purple sand pottery by using Jiangchuan siliceous sandstone and firing method
Europäisches Patentamt | 2021
|