Jianshui pottery firewood-fired pug formula and firing process
The invention discloses a Jianshui pottery firewood-fired pug formula and a firing process. The Jianshui pottery firewood-fired pug formula comprises the following raw materials in percentage by mass: 60.0%-70.0% of Jianshui white mud, 10%-15.0% of albite, 5.0%-15.0% of quartz sand and 5.0%-10.0% of volcanic mud. According to the firewood-fired clay for the Jianshui pottery, the firing temperature of the Jianshui pottery and the stability of the Jianshui pottery in the firing process can be effectively and remarkably improved, so that more high-quality firewood-fired products of the Jianshui pottery are prepared, in addition, by adding materials such as quartz sand, albite and volcanic mud, the formula and the firing process of the firewood-fired clay for the Jianshui pottery are improved, the high temperature resistance and the stability are very outstanding, albite and volcanic mud have the characteristic of lower melting temperature and can synchronously act on ash on the surfaces of firewood and pottery, so that the firewood and the pottery are easier to melt and form uniform and frizz-free glaze surfaces, and meanwhile, the energy consumption and the man-hour cost in the firing process can be greatly reduced; and the influence of the production of the building water pottery on the environment can be effectively reduced by using the conventional firewood firing.
本发明公开了一种建水陶柴烧泥料配方及烧制工艺,包括以下百分比质量份数原料:建水白泥60.0%‑70.0%、钠长石10%‑15.0%、石英砂5.0%‑15.0%和火山泥5.0%‑10.0%。能有效显著的提高了建水陶的烧成温度和烧制过程中的稳定性,从而制得更多的高品质建水陶柴烧产品,此外,通过添加石英砂、钠长石和火山泥等材料,改进了建水陶柴烧泥料配方及烧制工艺,其中,石英砂硬度极高,耐高温和稳定性能非常突出,钠长石和火山泥则具有熔融温度较低的特性,能够同步作用于薪柴和陶器表面的灰烬,使其更容易熔化,并形成均匀、无毛躁的釉面,同时还能大幅度减少烧制过程中的能耗和工时成本,利用常规的柴火烧制还可以有效地减少建水陶生产对环境的影响。
Jianshui pottery firewood-fired pug formula and firing process
The invention discloses a Jianshui pottery firewood-fired pug formula and a firing process. The Jianshui pottery firewood-fired pug formula comprises the following raw materials in percentage by mass: 60.0%-70.0% of Jianshui white mud, 10%-15.0% of albite, 5.0%-15.0% of quartz sand and 5.0%-10.0% of volcanic mud. According to the firewood-fired clay for the Jianshui pottery, the firing temperature of the Jianshui pottery and the stability of the Jianshui pottery in the firing process can be effectively and remarkably improved, so that more high-quality firewood-fired products of the Jianshui pottery are prepared, in addition, by adding materials such as quartz sand, albite and volcanic mud, the formula and the firing process of the firewood-fired clay for the Jianshui pottery are improved, the high temperature resistance and the stability are very outstanding, albite and volcanic mud have the characteristic of lower melting temperature and can synchronously act on ash on the surfaces of firewood and pottery, so that the firewood and the pottery are easier to melt and form uniform and frizz-free glaze surfaces, and meanwhile, the energy consumption and the man-hour cost in the firing process can be greatly reduced; and the influence of the production of the building water pottery on the environment can be effectively reduced by using the conventional firewood firing.
本发明公开了一种建水陶柴烧泥料配方及烧制工艺,包括以下百分比质量份数原料:建水白泥60.0%‑70.0%、钠长石10%‑15.0%、石英砂5.0%‑15.0%和火山泥5.0%‑10.0%。能有效显著的提高了建水陶的烧成温度和烧制过程中的稳定性,从而制得更多的高品质建水陶柴烧产品,此外,通过添加石英砂、钠长石和火山泥等材料,改进了建水陶柴烧泥料配方及烧制工艺,其中,石英砂硬度极高,耐高温和稳定性能非常突出,钠长石和火山泥则具有熔融温度较低的特性,能够同步作用于薪柴和陶器表面的灰烬,使其更容易熔化,并形成均匀、无毛躁的釉面,同时还能大幅度减少烧制过程中的能耗和工时成本,利用常规的柴火烧制还可以有效地减少建水陶生产对环境的影响。
Jianshui pottery firewood-fired pug formula and firing process
一种建水陶柴烧泥料配方及烧制工艺
FEI XINHUA (Autor:in)
14.07.2023
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Firewood firing method capable of firing Jianshui purple pottery with jade effect
Europäisches Patentamt | 2024
|Pottery firing process based on reverse flame type firewood firing dragon kiln
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2020
|