The invention discloses a cement-free novel high-strength ceramic tile adhesive. The formula of the cement-free novel high-strength ceramic tile adhesive comprises the following components in percentage by mass: 20-30% of slag powder; 20%-25% of steel slag powder; the desulfurized gypsum accounts for 45%-50%; 0.5%-1% of organic rubber powder; 0.5%-1% of cellulose ether; and 2%-3% of fly ash. According to the ceramic tile adhesive, the situation that cement is used as a formula raw material is removed, and the adhesive performance, the use strength and the use stability of the whole ceramic tile adhesive are improved through other formula raw materials such as the desulfurized gypsum, the organic rubber powder and the cellulose ether, so that the ceramic tile adhesive has high strength and high adhesive performance; on the one hand, the raw material cost of the novel high-strength ceramic tile adhesive free of addition of cement can be greatly reduced, on the other hand, the solid waste is adopted in the raw materials of the formula, the solid waste is reutilized, the cost of the raw materials of the formula is further reduced, resources are saved, distribution and utilization of the resources are optimized, and meanwhile the environment protection effect is achieved; and the method has huge social and economic benefits.
本申请公开一种免加水泥的新型高强度瓷砖胶,该免加水泥的新型高强度瓷砖胶的配方按照质量百分比为:矿渣粉为20%~30%;钢渣粉为20%~25%;脱硫石膏为45%~50%;有机胶粉0.5%~1%;纤维素醚为0.5%~1%;粉煤灰2%~3%。该瓷砖胶去除水泥作为配方原料的情况,通过其他诸如脱硫石膏、有机胶粉、纤维素醚等配方原料来改善整个瓷砖胶的胶粘性能以及使用的强度和稳定性,使瓷砖胶具有高强度和高胶粘性能,一方面由于去除了水泥的使用,可以大大降低免加水泥的新型高强度瓷砖胶配制的原料成本,另一方面,配方原料中采用了固体废料,对固体废料进行二次利用,不仅进一步降低了配方原料的成本,还节约了资源,优化了资源的分配和利用,同时也起到了环境保护的作用,具有巨大的社会经济效益。
Novel high-strength ceramic tile glue without adding cement
The invention discloses a cement-free novel high-strength ceramic tile adhesive. The formula of the cement-free novel high-strength ceramic tile adhesive comprises the following components in percentage by mass: 20-30% of slag powder; 20%-25% of steel slag powder; the desulfurized gypsum accounts for 45%-50%; 0.5%-1% of organic rubber powder; 0.5%-1% of cellulose ether; and 2%-3% of fly ash. According to the ceramic tile adhesive, the situation that cement is used as a formula raw material is removed, and the adhesive performance, the use strength and the use stability of the whole ceramic tile adhesive are improved through other formula raw materials such as the desulfurized gypsum, the organic rubber powder and the cellulose ether, so that the ceramic tile adhesive has high strength and high adhesive performance; on the one hand, the raw material cost of the novel high-strength ceramic tile adhesive free of addition of cement can be greatly reduced, on the other hand, the solid waste is adopted in the raw materials of the formula, the solid waste is reutilized, the cost of the raw materials of the formula is further reduced, resources are saved, distribution and utilization of the resources are optimized, and meanwhile the environment protection effect is achieved; and the method has huge social and economic benefits.
本申请公开一种免加水泥的新型高强度瓷砖胶,该免加水泥的新型高强度瓷砖胶的配方按照质量百分比为:矿渣粉为20%~30%;钢渣粉为20%~25%;脱硫石膏为45%~50%;有机胶粉0.5%~1%;纤维素醚为0.5%~1%;粉煤灰2%~3%。该瓷砖胶去除水泥作为配方原料的情况,通过其他诸如脱硫石膏、有机胶粉、纤维素醚等配方原料来改善整个瓷砖胶的胶粘性能以及使用的强度和稳定性,使瓷砖胶具有高强度和高胶粘性能,一方面由于去除了水泥的使用,可以大大降低免加水泥的新型高强度瓷砖胶配制的原料成本,另一方面,配方原料中采用了固体废料,对固体废料进行二次利用,不仅进一步降低了配方原料的成本,还节约了资源,优化了资源的分配和利用,同时也起到了环境保护的作用,具有巨大的社会经济效益。
Novel high-strength ceramic tile glue without adding cement
一种免加水泥的新型高强度瓷砖胶
HUANG WENFEI (Autor:in) / DONG QIYOU (Autor:in) / LIU WEI (Autor:in) / REN HAI (Autor:in)
15.07.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Aggregate for ceramic tile glue, preparation method of aggregate and ceramic tile glue
Europäisches Patentamt | 2023
|