Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Homogeneous autoclaved thermal insulation aerated building block produced by using waste rock wool powder
The invention discloses a homogeneous autoclaved thermal insulation aerated building block produced by using waste rock wool powder. The aerated building block is prepared from the following raw materials in parts by weight: 15 to 25 parts of cement, 3 to 7 parts of lime, 51 to 85 parts of mortar, 2 to 4 parts of gypsum, 1.5 to 2.5 parts of waste rock wool powder, 2 to 4 parts of furnace slag, 0.3 to 0.7 part of curing agent, 0.3 to 0.7 part of water reducing agent and 0.05 to 0.2 part of aluminum powder. According to the aerated building block, the waste rock wool powder is doped into the autoclaved aerated building block, so that the heat preservation effect of the autoclaved aerated building block is improved, the heat conductivity coefficient of the autoclaved aerated building block is reduced, the homogeneous heat preservation aerated building block meeting the design requirement is formed, meanwhile, the waste rock wool powder is uniformly distributed in the aerated building block, and the heat preservation aerated building block is formed; the thermal insulation effect of the building block and the overall quality of the thermal insulation building block are improved, good market benefits are achieved, the practical value is high, and the building block is suitable for application and popularization.
本发明公开了一种利用废旧岩棉粉生产匀质蒸压保温加气砌块。本发明所述的加气砌块,其原料按重量份包括:水泥15‑25份、石灰3‑7份、砂浆51‑85份、石膏2‑4份、废旧岩棉粉1.5‑2.5份、炉渣2‑4份、固化剂0.3‑0.7份、减水剂0.3‑0.7份、铝粉0.05‑0.2份。本发明所述加气砌块在蒸压加砌块中掺入废旧岩棉粉合二为一提高蒸压加砌块的保温效果,降低其导热系数形成符合设计要求的匀质保温加砌块,同时让废旧岩棉粉均匀分布在加砌块内部,形成保温加砌块,提高砌块的保温效果以及保温砌块整体的质量,具有良好的市场效益,实用性价值较高,适合推广使用。
Homogeneous autoclaved thermal insulation aerated building block produced by using waste rock wool powder
The invention discloses a homogeneous autoclaved thermal insulation aerated building block produced by using waste rock wool powder. The aerated building block is prepared from the following raw materials in parts by weight: 15 to 25 parts of cement, 3 to 7 parts of lime, 51 to 85 parts of mortar, 2 to 4 parts of gypsum, 1.5 to 2.5 parts of waste rock wool powder, 2 to 4 parts of furnace slag, 0.3 to 0.7 part of curing agent, 0.3 to 0.7 part of water reducing agent and 0.05 to 0.2 part of aluminum powder. According to the aerated building block, the waste rock wool powder is doped into the autoclaved aerated building block, so that the heat preservation effect of the autoclaved aerated building block is improved, the heat conductivity coefficient of the autoclaved aerated building block is reduced, the homogeneous heat preservation aerated building block meeting the design requirement is formed, meanwhile, the waste rock wool powder is uniformly distributed in the aerated building block, and the heat preservation aerated building block is formed; the thermal insulation effect of the building block and the overall quality of the thermal insulation building block are improved, good market benefits are achieved, the practical value is high, and the building block is suitable for application and popularization.
本发明公开了一种利用废旧岩棉粉生产匀质蒸压保温加气砌块。本发明所述的加气砌块,其原料按重量份包括:水泥15‑25份、石灰3‑7份、砂浆51‑85份、石膏2‑4份、废旧岩棉粉1.5‑2.5份、炉渣2‑4份、固化剂0.3‑0.7份、减水剂0.3‑0.7份、铝粉0.05‑0.2份。本发明所述加气砌块在蒸压加砌块中掺入废旧岩棉粉合二为一提高蒸压加砌块的保温效果,降低其导热系数形成符合设计要求的匀质保温加砌块,同时让废旧岩棉粉均匀分布在加砌块内部,形成保温加砌块,提高砌块的保温效果以及保温砌块整体的质量,具有良好的市场效益,实用性价值较高,适合推广使用。
Homogeneous autoclaved thermal insulation aerated building block produced by using waste rock wool powder
一种利用废旧岩棉粉生产匀质蒸压保温加气砌块
AN MINGYIN (Autor:in) / LYU JIHAI (Autor:in) / ZHU YOUJUN (Autor:in) / CHEN SHIYONG (Autor:in)
04.11.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2016
|Building material produced by using waste autoclaved aerated concrete product
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2023
|