The invention discloses a concrete formula and a concrete communication pole tower prepared from the concrete formula, the concrete formula is prepared from the following raw materials in percentage by mass: 22.43%-22.81% of Portland cement, 3.80%-5.42% of silicon powder, 36.3%-38.02% of pebbles, 29.04%-30.42% of sand and 4.53%-5.07% of water, and the sum of the mass percentages of the Portland cement, the silicon powder, the pebbles, the sand and the water is 100%. The tower body of the communication pole tower is formed by assembling the cement pole prepared by the concrete formula, by utilizing the formula, the strength of the cement pole tower is improved, the strength requirement of the communication pole tower is met, compared with a traditional steel structure pole tower, the production cost of the communication pole tower is reduced, and the tower body prepared by the cement pole tower has the advantages that the bending strength and the torsional strength are improved, and the service life of the communication pole tower is prolonged. The wind resistance is reduced, the occupied area is reduced, and the device can adapt to a complex installation environment.
本发明公开了一种混凝土配方及其制备的混凝土通信杆塔,其中混凝土配方包括由下列各组分质量百分比的原料加工而成:硅酸盐水泥22.43%‑22.81%、硅粉3.80%‑5.42%、石子36.3%‑38.02%、砂29.04%‑30.42%和水4.53%‑5.07%,其中硅酸盐水泥、硅粉、石子、砂和水的质量百分比之和为100%,该通信杆塔的塔体由该混凝土配方制备的水泥电杆组装而成,利用该配方,提高了水泥电杆的强度,满足通信杆塔的强度要求,相较于传统的钢结构杆塔,降低了通信杆塔的生产成为,且该水泥电杆制备的塔体提高了抗弯、抗扭强度,降低了风阻,减小了占地面积,能够适应复杂的安装环境。
Concrete formula and concrete communication tower prepared from concrete formula
The invention discloses a concrete formula and a concrete communication pole tower prepared from the concrete formula, the concrete formula is prepared from the following raw materials in percentage by mass: 22.43%-22.81% of Portland cement, 3.80%-5.42% of silicon powder, 36.3%-38.02% of pebbles, 29.04%-30.42% of sand and 4.53%-5.07% of water, and the sum of the mass percentages of the Portland cement, the silicon powder, the pebbles, the sand and the water is 100%. The tower body of the communication pole tower is formed by assembling the cement pole prepared by the concrete formula, by utilizing the formula, the strength of the cement pole tower is improved, the strength requirement of the communication pole tower is met, compared with a traditional steel structure pole tower, the production cost of the communication pole tower is reduced, and the tower body prepared by the cement pole tower has the advantages that the bending strength and the torsional strength are improved, and the service life of the communication pole tower is prolonged. The wind resistance is reduced, the occupied area is reduced, and the device can adapt to a complex installation environment.
本发明公开了一种混凝土配方及其制备的混凝土通信杆塔,其中混凝土配方包括由下列各组分质量百分比的原料加工而成:硅酸盐水泥22.43%‑22.81%、硅粉3.80%‑5.42%、石子36.3%‑38.02%、砂29.04%‑30.42%和水4.53%‑5.07%,其中硅酸盐水泥、硅粉、石子、砂和水的质量百分比之和为100%,该通信杆塔的塔体由该混凝土配方制备的水泥电杆组装而成,利用该配方,提高了水泥电杆的强度,满足通信杆塔的强度要求,相较于传统的钢结构杆塔,降低了通信杆塔的生产成为,且该水泥电杆制备的塔体提高了抗弯、抗扭强度,降低了风阻,减小了占地面积,能够适应复杂的安装环境。
Concrete formula and concrete communication tower prepared from concrete formula
一种混凝土配方及其制备的混凝土通信杆塔
LI LIXIN (Autor:in) / WU YONG (Autor:in) / WANG XINXIN (Autor:in) / ZHANG YUEJUN (Autor:in) / SHEN ZHONGMING (Autor:in) / LIU HAO (Autor:in) / GUAN QINGXIANG (Autor:in) / CHEN XIAOWEI (Autor:in) / LI ZHONGQI (Autor:in) / YU YONGXIANG (Autor:in)