Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Resin carbon anode green body and preparation method thereof, green body intermediate and preparation method thereof, carbon anode and preparation method thereof
The invention provides a resin carbon anode green body, the resin carbon anode green body is subjected to hardening treatment to obtain a resin carbon anode green body intermediate, and when the resin carbon anode green body intermediate is tested through a gas chromatography-mass spectrometry technology, the resin carbon anode green body intermediate has the following spectrum characteristics that characteristic peaks exist at the retention time of 8.28 +/-0.3 min, 12.7 +/-0.3 min, 14.6 +/-0.3 min and 19.0 +/-0.3 min in sequence. The invention also provides a preparation method of the resin carbon anode green body. In addition, the invention further provides a resin carbon anode green body intermediate, a resin carbon anode and a corresponding preparation method and application of the resin carbon anode.
本申请提供了一种树脂炭素阳极生坯,所述树脂炭素阳极生坯经硬化处理后得树脂炭素阳极生坯中间体,所述树脂炭素阳极生坯中间体通过气相色谱‑质谱联用技术测试时具有以下图谱特征:在保留时间依次为8.28±0.3min、12.7±0.3min、14.6±0.3min和19.0±0.3min处有特征峰。本发明还提供了树脂炭素阳极生坯的制备方法。另外,本发明还提供了一种树脂炭素阳极生坯中间体、树脂炭素阳极及其相应的制备方法及应用。
Resin carbon anode green body and preparation method thereof, green body intermediate and preparation method thereof, carbon anode and preparation method thereof
The invention provides a resin carbon anode green body, the resin carbon anode green body is subjected to hardening treatment to obtain a resin carbon anode green body intermediate, and when the resin carbon anode green body intermediate is tested through a gas chromatography-mass spectrometry technology, the resin carbon anode green body intermediate has the following spectrum characteristics that characteristic peaks exist at the retention time of 8.28 +/-0.3 min, 12.7 +/-0.3 min, 14.6 +/-0.3 min and 19.0 +/-0.3 min in sequence. The invention also provides a preparation method of the resin carbon anode green body. In addition, the invention further provides a resin carbon anode green body intermediate, a resin carbon anode and a corresponding preparation method and application of the resin carbon anode.
本申请提供了一种树脂炭素阳极生坯,所述树脂炭素阳极生坯经硬化处理后得树脂炭素阳极生坯中间体,所述树脂炭素阳极生坯中间体通过气相色谱‑质谱联用技术测试时具有以下图谱特征:在保留时间依次为8.28±0.3min、12.7±0.3min、14.6±0.3min和19.0±0.3min处有特征峰。本发明还提供了树脂炭素阳极生坯的制备方法。另外,本发明还提供了一种树脂炭素阳极生坯中间体、树脂炭素阳极及其相应的制备方法及应用。
Resin carbon anode green body and preparation method thereof, green body intermediate and preparation method thereof, carbon anode and preparation method thereof
树脂炭素阳极生坯及制备方法、生坯中间体及制备方法、炭素阳极及制备方法