The invention provides an anti-static misfire wear-resistant floor material as well as a preparation method and a construction method thereof, and relates to the technical field of coating materials. The antistatic misfire wear-resistant floor material comprises a component A and a component B in a mass ratio of (4-7): 1, the component A comprises, by mass, 30-45% of cement, 45-55% of misfire aggregate, 1-3% of an active admixture, 5-10% of a functional additive, 0.5-1% of a special additive and 0.1-1.2% of a conductive material, and the component B is a polymer emulsion. The anti-static misfire wear-resistant floor material is a two-component polymer wear-resistant material, the bond energy of the material is improved through a cross-linking reaction of the emulsion, the cement and the active material, the balance of rigidity and flexibility is achieved, on one hand, the mechanical property of a finished product can be improved, and on the other hand, the anti-static misfire wear-resistant floor material is environment-friendly; on the other hand, the defects that a single-component anti-static misfire wear-resistant material is brittle and easy to crack are improved and avoided.
本发明提供一种防静电不发火耐磨地坪材料及其制备和施工方法,涉及涂料材料技术领域。一种防静电不发火耐磨地坪材料,包括质量比为(4‑7):1的A组份和B组份,A组份按质量分数计包括水泥30‑45%,不发火骨料45‑55%,活性掺和料1‑3%,功能外加剂5‑10%,特种外加剂0.5‑1%和导电材料0.1‑1.2%,B组份为聚合物乳液。本发明的防静电不发火耐磨地坪材料为双组份聚合物耐磨材料,通过乳液与水泥及活性材料发生交联反应提高材料键能,达到刚性和柔性的平衡,一方面可以提高成品的力学性能,另一方面改善和避免了单组份防静电不发火耐磨材料性脆易开裂的缺点。
Anti-static misfire wear-resistant floor material as well as preparation and construction methods thereof
The invention provides an anti-static misfire wear-resistant floor material as well as a preparation method and a construction method thereof, and relates to the technical field of coating materials. The antistatic misfire wear-resistant floor material comprises a component A and a component B in a mass ratio of (4-7): 1, the component A comprises, by mass, 30-45% of cement, 45-55% of misfire aggregate, 1-3% of an active admixture, 5-10% of a functional additive, 0.5-1% of a special additive and 0.1-1.2% of a conductive material, and the component B is a polymer emulsion. The anti-static misfire wear-resistant floor material is a two-component polymer wear-resistant material, the bond energy of the material is improved through a cross-linking reaction of the emulsion, the cement and the active material, the balance of rigidity and flexibility is achieved, on one hand, the mechanical property of a finished product can be improved, and on the other hand, the anti-static misfire wear-resistant floor material is environment-friendly; on the other hand, the defects that a single-component anti-static misfire wear-resistant material is brittle and easy to crack are improved and avoided.
本发明提供一种防静电不发火耐磨地坪材料及其制备和施工方法,涉及涂料材料技术领域。一种防静电不发火耐磨地坪材料,包括质量比为(4‑7):1的A组份和B组份,A组份按质量分数计包括水泥30‑45%,不发火骨料45‑55%,活性掺和料1‑3%,功能外加剂5‑10%,特种外加剂0.5‑1%和导电材料0.1‑1.2%,B组份为聚合物乳液。本发明的防静电不发火耐磨地坪材料为双组份聚合物耐磨材料,通过乳液与水泥及活性材料发生交联反应提高材料键能,达到刚性和柔性的平衡,一方面可以提高成品的力学性能,另一方面改善和避免了单组份防静电不发火耐磨材料性脆易开裂的缺点。
Anti-static misfire wear-resistant floor material as well as preparation and construction methods thereof
一种防静电不发火耐磨地坪材料及其制备和施工方法
HUANG LISHENG (Autor:in)
20.10.2023
Patent
Elektronische Ressource
Chinesisch
Anti-static misfire metal wear-resistant floor material and preparation method thereof
Europäisches Patentamt | 2021
|Anti-static misfire metal wear-resistant floor material and preparation method thereof
Europäisches Patentamt | 2022
|Europäisches Patentamt | 2022
|Highly wear-resistant floor material and construction method thereof
Europäisches Patentamt | 2022
|