Concrete slurry and preparation method thereof, and application of concrete and polymer
The invention discloses concrete slurry which comprises the following components in parts by weight: 285 parts of cement, 20-50 parts of fly ash, 613-750 parts of sand, 950-1150 parts of gravel, 85-120 parts of slag powder, 4-15 parts of a polymer, 20-45 parts of an expanding agent and water, wherein the polymer is obtained by carrying out polymerization reaction on raw materials including isopentenol polyoxyethylene ether, acrylic acid and gamma-aminopropyltriethoxysilane; the number-average molecular weight of the isopentenol polyoxyethylene ether is 2100 to 2800, and the molar ratio of the isopentenol polyoxyethylene ether to the acrylic acid to the gamma-aminopropyltriethoxysilane is 1: (3 to 6): (0.05 to 0.5). The concrete slurry is less in hydration heat release and relatively slow in hydration heat release rate.
本发明公开了一种混凝土浆料,包括:水泥285重量份、粉煤灰20~50重量份、砂613~750重量份、碎石950~1150重量份、矿渣粉85~120重量份、聚合物4~15重量份、20~45重量份膨胀剂和水;其中,所述聚合物由包括异戊烯醇聚氧乙烯醚、丙烯酸和γ‑氨丙基三乙氧基硅烷的原料经聚合反应得到;所述异戊烯醇聚氧乙烯醚的数均分子量为2100~2800,所述异戊烯醇聚氧乙烯醚、丙烯酸和γ‑氨丙基三乙氧基硅烷的摩尔比为1:(3~6):(0.05~0.5)。该混凝土浆料水化放热少,水化放热速率较慢。
Concrete slurry and preparation method thereof, and application of concrete and polymer
The invention discloses concrete slurry which comprises the following components in parts by weight: 285 parts of cement, 20-50 parts of fly ash, 613-750 parts of sand, 950-1150 parts of gravel, 85-120 parts of slag powder, 4-15 parts of a polymer, 20-45 parts of an expanding agent and water, wherein the polymer is obtained by carrying out polymerization reaction on raw materials including isopentenol polyoxyethylene ether, acrylic acid and gamma-aminopropyltriethoxysilane; the number-average molecular weight of the isopentenol polyoxyethylene ether is 2100 to 2800, and the molar ratio of the isopentenol polyoxyethylene ether to the acrylic acid to the gamma-aminopropyltriethoxysilane is 1: (3 to 6): (0.05 to 0.5). The concrete slurry is less in hydration heat release and relatively slow in hydration heat release rate.
本发明公开了一种混凝土浆料,包括:水泥285重量份、粉煤灰20~50重量份、砂613~750重量份、碎石950~1150重量份、矿渣粉85~120重量份、聚合物4~15重量份、20~45重量份膨胀剂和水;其中,所述聚合物由包括异戊烯醇聚氧乙烯醚、丙烯酸和γ‑氨丙基三乙氧基硅烷的原料经聚合反应得到;所述异戊烯醇聚氧乙烯醚的数均分子量为2100~2800,所述异戊烯醇聚氧乙烯醚、丙烯酸和γ‑氨丙基三乙氧基硅烷的摩尔比为1:(3~6):(0.05~0.5)。该混凝土浆料水化放热少,水化放热速率较慢。
Concrete slurry and preparation method thereof, and application of concrete and polymer
混凝土浆料及其制备方法、混凝土和聚合物的用途
CHANG NAIKUN (Autor:in) / HE XUECHUN (Autor:in) / JIANG YANYAN (Autor:in) / DONG XIANGJUN (Autor:in) / GAO ZONGZHI (Autor:in) / HE XIANG (Autor:in) / MA XIUCI (Autor:in) / LIU HANG (Autor:in) / PENG CHAO (Autor:in)
27.10.2023
Patent
Elektronische Ressource
Chinesisch
Concrete waste slurry treatment process and concrete preparation method thereof
Europäisches Patentamt | 2023
|Waste slurry powder concrete and preparation method thereof
Europäisches Patentamt | 2021
|Concrete slurry homogenizing regulator as well as preparation method and application thereof
Europäisches Patentamt | 2024
|Slurry-coated reinforced permeable recycled concrete and preparation method thereof
Europäisches Patentamt | 2021
|