The invention relates to a cement stabilized macadam mixture doped with waste incineration slag. The mixture is prepared from the following components in parts by weight: 50-100 parts of slag; 60 to 200 parts by weight of cement; 10 to 80 parts by weight of rock; 10 to 40 parts by weight of gypsum; 20 to 60 parts by weight of fly ash; 10 to 30 parts by weight of a cementing agent; and 20-70 parts by weight of metal powder. In the invention, when the slag, the cement, the rock, the gypsum, the fly ash, the cementing agent and the metal powder are mixed for production, the produced mixture is the best, and the mixed brick produced from the mixture has the best compression resistance and bending resistance and can be popularized and used. In addition, by adding the metal powder, the bending resistance and the compression resistance of the brick C can be greatly improved.
本发明涉及一种掺入垃圾焚烧炉渣的水泥稳定碎石混合料,所述混合料按照重量份由以下成分组分:炉渣:50‑100重量份;水泥:60‑200重量份;岩石:10‑80重量份;石膏:10‑40重量份;粉煤灰:20‑60重量份;胶结剂:10‑30重量份;金属粉:20‑70重量份。本发明中,通过当炉渣、水泥、岩石、石膏、粉煤灰、胶结剂以及金属粉混合生产时,生产出的混合料最好,而由混合料生产出来的混合砖块的抗压性能以及抗弯性能效果最好,可以推广使用。且本发明中,通过金属粉的添加,能够大大提高砖块C的抗弯性能以及抗压性能。
Cement stabilized macadam mixture doped with waste incineration slag
The invention relates to a cement stabilized macadam mixture doped with waste incineration slag. The mixture is prepared from the following components in parts by weight: 50-100 parts of slag; 60 to 200 parts by weight of cement; 10 to 80 parts by weight of rock; 10 to 40 parts by weight of gypsum; 20 to 60 parts by weight of fly ash; 10 to 30 parts by weight of a cementing agent; and 20-70 parts by weight of metal powder. In the invention, when the slag, the cement, the rock, the gypsum, the fly ash, the cementing agent and the metal powder are mixed for production, the produced mixture is the best, and the mixed brick produced from the mixture has the best compression resistance and bending resistance and can be popularized and used. In addition, by adding the metal powder, the bending resistance and the compression resistance of the brick C can be greatly improved.
本发明涉及一种掺入垃圾焚烧炉渣的水泥稳定碎石混合料,所述混合料按照重量份由以下成分组分:炉渣:50‑100重量份;水泥:60‑200重量份;岩石:10‑80重量份;石膏:10‑40重量份;粉煤灰:20‑60重量份;胶结剂:10‑30重量份;金属粉:20‑70重量份。本发明中,通过当炉渣、水泥、岩石、石膏、粉煤灰、胶结剂以及金属粉混合生产时,生产出的混合料最好,而由混合料生产出来的混合砖块的抗压性能以及抗弯性能效果最好,可以推广使用。且本发明中,通过金属粉的添加,能够大大提高砖块C的抗弯性能以及抗压性能。
Cement stabilized macadam mixture doped with waste incineration slag
一种掺入垃圾焚烧炉渣的水泥稳定碎石混合料
PANG SHUTAO (Autor:in) / ZHAO YONG (Autor:in) / LIU SHULONG (Autor:in)
01.12.2023
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Cement stabilized macadam mixture doped with waste incineration slag
Europäisches Patentamt | 2020
|Method for using household garbage incineration slag as cement stabilized macadam base
Europäisches Patentamt | 2024
|Application of household garbage incineration fly ash in cement stabilized macadam mixture
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2024
|