Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Brick making formula based on dredged sludge, process and application
The invention discloses a brick making formula based on dredged sludge, a process and application, the formula mainly selects dredged sludge, and cement, fly ash, slag, gypsum, lime, a water reducing agent and an early strength agent are added to form a specific formula system, so that not only can energy be saved, but also a river channel can be dredged, and waste is turned into wealth; a proper way is explored for reasonable treatment and utilization of industrial waste, and the economic benefit, the social benefit and the environmental benefit are very remarkable. Through the independently researched and developed specific formula and process, the compressive strength and breaking strength of the sludge brick product are improved, and the impermeability and erosion resistance of the sludge brick product are optimized. Moreover, the high-standard requirement in the industry can be met by curing the sludge brick prepared by the process for 7-14 days, the traditional 28-day curing period standard is broken, the curing time and the production period are reduced, the process efficiency is greatly improved, and the process has excellent market popularization and application prospects.
本发明公布了基于疏浚淤泥的制砖配方、工艺及应用,配方主要选用疏浚淤泥,添加水泥、粉煤灰、矿渣、石膏、石灰、减水剂及早强剂构成了特定配方体系,不但可以节约能源,还能疏通河道、变废为宝,为工业废料的合理化处理及利用探寻了合适的途径,经济效益、社会效益及环境效益都十分显著。通过自主研发的特定配方和工艺,提高了淤泥砖制品的抗压强度和抗折强度,并优化其抗渗抗侵蚀性能。而且,通过本发明的工艺制备淤泥砖,养护7~14天即可满足行业内的高标准要求,打破了传统的28天养护期标准,减少了养护时间和生产周期,大大提高了工艺效率,具有极好的市场化推广应用前景。
Brick making formula based on dredged sludge, process and application
The invention discloses a brick making formula based on dredged sludge, a process and application, the formula mainly selects dredged sludge, and cement, fly ash, slag, gypsum, lime, a water reducing agent and an early strength agent are added to form a specific formula system, so that not only can energy be saved, but also a river channel can be dredged, and waste is turned into wealth; a proper way is explored for reasonable treatment and utilization of industrial waste, and the economic benefit, the social benefit and the environmental benefit are very remarkable. Through the independently researched and developed specific formula and process, the compressive strength and breaking strength of the sludge brick product are improved, and the impermeability and erosion resistance of the sludge brick product are optimized. Moreover, the high-standard requirement in the industry can be met by curing the sludge brick prepared by the process for 7-14 days, the traditional 28-day curing period standard is broken, the curing time and the production period are reduced, the process efficiency is greatly improved, and the process has excellent market popularization and application prospects.
本发明公布了基于疏浚淤泥的制砖配方、工艺及应用,配方主要选用疏浚淤泥,添加水泥、粉煤灰、矿渣、石膏、石灰、减水剂及早强剂构成了特定配方体系,不但可以节约能源,还能疏通河道、变废为宝,为工业废料的合理化处理及利用探寻了合适的途径,经济效益、社会效益及环境效益都十分显著。通过自主研发的特定配方和工艺,提高了淤泥砖制品的抗压强度和抗折强度,并优化其抗渗抗侵蚀性能。而且,通过本发明的工艺制备淤泥砖,养护7~14天即可满足行业内的高标准要求,打破了传统的28天养护期标准,减少了养护时间和生产周期,大大提高了工艺效率,具有极好的市场化推广应用前景。
Brick making formula based on dredged sludge, process and application
基于疏浚淤泥的制砖配方、工艺及应用
ZHANG JIAN (Autor:in) / HU CHENCHEN (Autor:in) / ZHANG WENBIN (Autor:in)
29.12.2023
Patent
Elektronische Ressource
Chinesisch
Building sludge comprehensive brick making process and brick
Europäisches Patentamt | 2022
|Sludge-to-brick method process and brick making process system
Europäisches Patentamt | 2021
|River and lake sludge brick making process and brick making equipment thereof
Europäisches Patentamt | 2023
|