Low-carbon high-iron sulphoaluminate cementing material produced from solid waste steel slag and preparation method of low-carbon high-iron sulphoaluminate cementing material
The invention relates to the technical field of cementitious material production, in particular to a low-carbon high-iron sulphoaluminate cementitious material produced from solid waste steel slag and a preparation method thereof.The cementitious material is mainly prepared from, by weight, 35-55% of limestone, 5-10% of anhydrite, 5-10% of bauxite and 5-10% of steel slag. The weight ratio of the anhydrite is 10-20%, the weight ratio of the bauxite is 20-45%, and the weight ratio of the steel slag is 5-20%. By arranging the elastic bag, the cover plate, the connecting rope, the lifting ring and other components, in the operation process of the equipment, the elastic bag is extruded through the grinding rod, then the cover plate is moved, and the cover plate is moved; the angle of the smashing cutter is deflected under the cooperation of the connecting rope, then the smashing effect of the smashing cutter is changed, the lifting ring descends, and the discharging hole is reduced and unblocked under the cooperation of the scraping hole and the discharging hole, so that the grinding effect on the grinding disc is guaranteed.
本发明涉及胶凝材料生产的技术领域,特别是涉及一种固废钢渣生产低碳高铁硫铝酸盐胶凝材料及制备方法,其所述胶凝材料主要由以下原料制备而成:石灰石、硬石膏、铝矾土和钢渣,其中,所述石灰石占配重比为35‑55%,所述硬石膏占配重比为10‑20%,所述铝矾土占配重比为20‑45%,所述钢渣占配重比为5‑20%,本发明通过设置弹性囊、盖板、连接绳和升降圈等部件,使设备在进行运转的过程中,通过研磨杆对弹性囊进行挤压,进而使盖板移动,在连接绳的配合下使粉碎刀的角度偏转,进而改变粉碎刀的粉碎效果,并且使升降圈下降,在刮料孔与排料孔的配合下使排料孔减小和使排料孔清堵,以保证研磨盘上的研磨效果。
Low-carbon high-iron sulphoaluminate cementing material produced from solid waste steel slag and preparation method of low-carbon high-iron sulphoaluminate cementing material
The invention relates to the technical field of cementitious material production, in particular to a low-carbon high-iron sulphoaluminate cementitious material produced from solid waste steel slag and a preparation method thereof.The cementitious material is mainly prepared from, by weight, 35-55% of limestone, 5-10% of anhydrite, 5-10% of bauxite and 5-10% of steel slag. The weight ratio of the anhydrite is 10-20%, the weight ratio of the bauxite is 20-45%, and the weight ratio of the steel slag is 5-20%. By arranging the elastic bag, the cover plate, the connecting rope, the lifting ring and other components, in the operation process of the equipment, the elastic bag is extruded through the grinding rod, then the cover plate is moved, and the cover plate is moved; the angle of the smashing cutter is deflected under the cooperation of the connecting rope, then the smashing effect of the smashing cutter is changed, the lifting ring descends, and the discharging hole is reduced and unblocked under the cooperation of the scraping hole and the discharging hole, so that the grinding effect on the grinding disc is guaranteed.
本发明涉及胶凝材料生产的技术领域,特别是涉及一种固废钢渣生产低碳高铁硫铝酸盐胶凝材料及制备方法,其所述胶凝材料主要由以下原料制备而成:石灰石、硬石膏、铝矾土和钢渣,其中,所述石灰石占配重比为35‑55%,所述硬石膏占配重比为10‑20%,所述铝矾土占配重比为20‑45%,所述钢渣占配重比为5‑20%,本发明通过设置弹性囊、盖板、连接绳和升降圈等部件,使设备在进行运转的过程中,通过研磨杆对弹性囊进行挤压,进而使盖板移动,在连接绳的配合下使粉碎刀的角度偏转,进而改变粉碎刀的粉碎效果,并且使升降圈下降,在刮料孔与排料孔的配合下使排料孔减小和使排料孔清堵,以保证研磨盘上的研磨效果。
Low-carbon high-iron sulphoaluminate cementing material produced from solid waste steel slag and preparation method of low-carbon high-iron sulphoaluminate cementing material
一种固废钢渣生产低碳高铁硫铝酸盐胶凝材料及制备方法
ZHANG SHIJIE (Autor:in) / LI HAO (Autor:in) / ZHANG XUEWEN (Autor:in) / LIU XIAOFEN (Autor:in) / LIANG JINGJIE (Autor:in)
04.06.2024
Patent
Elektronische Ressource
Chinesisch
Europäisches Patentamt | 2022
|Europäisches Patentamt | 2024
|Europäisches Patentamt | 2021
|Europäisches Patentamt | 2023
|