Dry-process high-viscosity modified asphalt mixture
The invention discloses a dry-process high-viscosity modified asphalt mixture, and belongs to the technical field. The technical problems that the existing high-viscosity high-elasticity modified asphalt is long in storage time and unstable in performance during high-temperature storage are solved. The dry-method high-viscosity modified asphalt mixture provided by the invention is prepared from the following components in parts by mass: 86.7 to 92.6 parts of aggregate, 3 to 8 parts of mineral powder, 0.4 to 0.8 part of high-viscosity modifier and 4.0 to 4.5 parts of asphalt. The high-viscosity and high-elasticity modifier can be placed at normal temperature, can be used at any time and is stable in performance, and a dry-process type high-viscosity modified asphalt mixture prepared from the high-viscosity and high-elasticity modifier is also stable in performance.
本发明公开了一种干法型高粘改性沥青混合料,属于技术领域;解决了现有高粘高弹改性沥青高温存储时,存储时间长且其性能不稳定的技术问题。本发明提供的干法型高粘改性沥青混合料按质量计包括:集料:86.7~92.6份,矿粉:3~8份,高粘改性剂:0.4~0.8份和沥青4.0~4.5份。本发明的高粘高弹改性剂可常温放置,随时可用,性能稳定,由其制备的干法型高粘改性沥青混合料也性能稳定。
Dry-process high-viscosity modified asphalt mixture
The invention discloses a dry-process high-viscosity modified asphalt mixture, and belongs to the technical field. The technical problems that the existing high-viscosity high-elasticity modified asphalt is long in storage time and unstable in performance during high-temperature storage are solved. The dry-method high-viscosity modified asphalt mixture provided by the invention is prepared from the following components in parts by mass: 86.7 to 92.6 parts of aggregate, 3 to 8 parts of mineral powder, 0.4 to 0.8 part of high-viscosity modifier and 4.0 to 4.5 parts of asphalt. The high-viscosity and high-elasticity modifier can be placed at normal temperature, can be used at any time and is stable in performance, and a dry-process type high-viscosity modified asphalt mixture prepared from the high-viscosity and high-elasticity modifier is also stable in performance.
本发明公开了一种干法型高粘改性沥青混合料,属于技术领域;解决了现有高粘高弹改性沥青高温存储时,存储时间长且其性能不稳定的技术问题。本发明提供的干法型高粘改性沥青混合料按质量计包括:集料:86.7~92.6份,矿粉:3~8份,高粘改性剂:0.4~0.8份和沥青4.0~4.5份。本发明的高粘高弹改性剂可常温放置,随时可用,性能稳定,由其制备的干法型高粘改性沥青混合料也性能稳定。
Dry-process high-viscosity modified asphalt mixture
一种干法型高粘改性沥青混合料
LEI WEI (Autor:in) / LIU JIAHUI (Autor:in) / PU CHANGYU (Autor:in) / WANG QINGKAI (Autor:in) / MENG HUILIN (Autor:in) / SUN CHAO (Autor:in) / MA HUABAO (Autor:in) / LUO YAN (Autor:in) / YUAN KUO (Autor:in) / GAI HUILIN (Autor:in)
16.07.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of dry-process high-viscosity modified asphalt mixture
Europäisches Patentamt | 2024
|High-viscosity modified asphalt mixture and application thereof
Europäisches Patentamt | 2020
|High-viscosity asphalt modifier, preparation method thereof, modified asphalt and asphalt mixture
Europäisches Patentamt | 2022
|High-viscosity modified volcanic slag adsorption type permeable asphalt mixture
Europäisches Patentamt | 2023
|Odorless high-viscosity asphalt modifier and asphalt mixture thereof
Europäisches Patentamt | 2020
|