The invention relates to the field of ceramic preparation, in particular to a smoky rain green glaze and a preparation method thereof. A unique formula is adopted, and the natural plant blue, the Pingding carclazyte and the bran ash are added into the glaze formula, are all mineral raw materials and do not contain heavy metal; the smoky rain cyan glaze is unique in formula, and the Pingding carclazyte and the bran ash are low in price, so that the cost can be reduced; the firing temperature is 1210-1270 DEG C, one-time firing is achieved, and compared with a traditional celadon manufacturing process, energy consumption is low, and cost can be saved. And the fired finished product porcelain has a fine and smooth glaze surface and a green and elegant glaze color, is just immersed in smoky rain, is implicit, quiet and quiet, and has an elegant effect.
本发明涉及陶瓷制备领域,具体涉及一种烟雨青釉料及其制备方法;本发明采用独特的配方组方,釉料组方中加入天然植物蓝,平定白土,糠灰,全部都是矿物原料,不含重金属;本发明的烟雨青釉配方独特,平定白土、糠灰价格低廉,可降低成本;本发明烧成温度为1210—1270℃,且一次烧成,与传统青瓷制作工艺相比,能源消耗低,可节省成本。烧成后的成品瓷釉面细腻光润,釉色青翠淡雅,似沉浸在烟雨中,含蓄、沉静、淡然,具有雅致的效果。
The invention relates to the field of ceramic preparation, in particular to a smoky rain green glaze and a preparation method thereof. A unique formula is adopted, and the natural plant blue, the Pingding carclazyte and the bran ash are added into the glaze formula, are all mineral raw materials and do not contain heavy metal; the smoky rain cyan glaze is unique in formula, and the Pingding carclazyte and the bran ash are low in price, so that the cost can be reduced; the firing temperature is 1210-1270 DEG C, one-time firing is achieved, and compared with a traditional celadon manufacturing process, energy consumption is low, and cost can be saved. And the fired finished product porcelain has a fine and smooth glaze surface and a green and elegant glaze color, is just immersed in smoky rain, is implicit, quiet and quiet, and has an elegant effect.
本发明涉及陶瓷制备领域,具体涉及一种烟雨青釉料及其制备方法;本发明采用独特的配方组方,釉料组方中加入天然植物蓝,平定白土,糠灰,全部都是矿物原料,不含重金属;本发明的烟雨青釉配方独特,平定白土、糠灰价格低廉,可降低成本;本发明烧成温度为1210—1270℃,且一次烧成,与传统青瓷制作工艺相比,能源消耗低,可节省成本。烧成后的成品瓷釉面细腻光润,釉色青翠淡雅,似沉浸在烟雨中,含蓄、沉静、淡然,具有雅致的效果。
Smoke rain green glaze and preparation method thereof
一种烟雨青釉料及其制备方法
24.09.2024
Patent
Elektronische Ressource
Chinesisch
Green background crystal glaze and preparation method thereof
Europäisches Patentamt | 2020
|Pea-green glaze porcelain and preparation method thereof
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2021
|