The invention discloses an early-strength micro-expansion underwater non-dispersible grouting material and a preparation method thereof. The early-strength micro-expansion underwater non-dispersible grouting material comprises the following components in parts by weight: 25-50 parts of Portland cement, 20-40 parts of sulphoaluminate cement, 5-30 parts of mineral powder, 5-30 parts of fine aggregate, 3-10 parts of microbeads, 0.3-2.5 parts of an anti-dispersing agent and 0.27-4 parts of a functional aid, and the sum of the parts by weight of all the components is 100. By implementing the preparation method, the prepared early-strength micro-expansion underwater non-dispersible grouting material has good mechanical properties and working properties and excellent underwater dispersion resistance and filling compactness.
本发明公开了一种早强微膨胀水下不分散灌浆料及其制备方法,所述早强微膨胀水下不分散灌浆料包括以下重量份的组分:硅酸盐水泥25~50份,硫铝酸盐水泥20~40份,矿粉5~30份,细集料5~30份,微珠3~10份,抗分散剂0.3~2.5份,功能助剂0.27~4份,各组分的重量份之和为100份。实施本发明,制备得到的早强微膨胀水下不分散灌浆料具备良好的力学性能、工作性能及优异的水下抗分散及填充密实性。
Early-strength micro-expansion underwater non-dispersible grouting material and preparation method thereof
The invention discloses an early-strength micro-expansion underwater non-dispersible grouting material and a preparation method thereof. The early-strength micro-expansion underwater non-dispersible grouting material comprises the following components in parts by weight: 25-50 parts of Portland cement, 20-40 parts of sulphoaluminate cement, 5-30 parts of mineral powder, 5-30 parts of fine aggregate, 3-10 parts of microbeads, 0.3-2.5 parts of an anti-dispersing agent and 0.27-4 parts of a functional aid, and the sum of the parts by weight of all the components is 100. By implementing the preparation method, the prepared early-strength micro-expansion underwater non-dispersible grouting material has good mechanical properties and working properties and excellent underwater dispersion resistance and filling compactness.
本发明公开了一种早强微膨胀水下不分散灌浆料及其制备方法,所述早强微膨胀水下不分散灌浆料包括以下重量份的组分:硅酸盐水泥25~50份,硫铝酸盐水泥20~40份,矿粉5~30份,细集料5~30份,微珠3~10份,抗分散剂0.3~2.5份,功能助剂0.27~4份,各组分的重量份之和为100份。实施本发明,制备得到的早强微膨胀水下不分散灌浆料具备良好的力学性能、工作性能及优异的水下抗分散及填充密实性。
Early-strength micro-expansion underwater non-dispersible grouting material and preparation method thereof
一种早强微膨胀水下不分散灌浆料及其制备方法
LI YONGLING (Autor:in) / YANG TENGYU (Autor:in) / QIU BING (Autor:in) / LEE BAEK-WOON (Autor:in) / CHENG HAO (Autor:in) / GUO LIXIAN (Autor:in) / LI MINGYANG (Autor:in) / ZHENG LISHANG (Autor:in)
29.10.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Micro-expansion grouting material for grouting with mold and preparation method thereof
Europäisches Patentamt | 2020
|Micro-expansion high-strength offshore wind power grouting material and preparation method thereof
Europäisches Patentamt | 2023
|Nano micro-expansion inorganic grouting material and preparation method thereof
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2023
|