Super-early-strength anticorrosive mortar and preparation method thereof
The invention discloses super-early-strength anticorrosive mortar and a preparation method thereof. The super early strength anticorrosive mortar is prepared from the following components in parts by weight: 400 to 500 parts of anticorrosive resin, 40 to 50 parts of plasticizer, 1 to 5 parts of defoaming agent, 25 to 35 parts of water repellent, 200 to 300 parts of solid waste micro powder, 200 to 300 parts of tailing sand, 100 to 150 parts of exciting agent, 5 to 10 parts of toughening fiber and 150 to 200 parts of water. According to the invention, the thermoplastic anticorrosive resin and the solid waste-based alkali-activated material are adopted as main cementing materials, so that the coating has the characteristics of short curing time, high early strength, acid and alkali corrosion resistance, water and oil corrosion resistance, high toughness and crack resistance, and is suitable for various corrosive environments; meanwhile, the solid waste is subjected to resource utilization, so that the cost is reduced, and secondary utilization of solid waste resources is facilitated.
本发明公开了一种超早强防腐砂浆及制备方法。本发明的超早强防腐砂浆,按重量份计,包括以下组分:防腐树脂400‑500份,增塑剂40‑50份,消泡剂1‑5份,憎水剂25‑35份,固废微粉200‑300份,尾矿砂200‑300份,激发剂100‑150份,增韧纤维5‑10份和水150‑200份。本发明采用热塑性防腐树脂和固废基碱激发材料作为主要胶凝材料,具有固化时间短,早期强度高、耐酸碱侵蚀、耐水油侵蚀、高韧性防裂的特点,适用于各种腐蚀性的环境中;同时由于对固废进行资源化利用,降低了成本,有利于推动固废资源二次利用。
Super-early-strength anticorrosive mortar and preparation method thereof
The invention discloses super-early-strength anticorrosive mortar and a preparation method thereof. The super early strength anticorrosive mortar is prepared from the following components in parts by weight: 400 to 500 parts of anticorrosive resin, 40 to 50 parts of plasticizer, 1 to 5 parts of defoaming agent, 25 to 35 parts of water repellent, 200 to 300 parts of solid waste micro powder, 200 to 300 parts of tailing sand, 100 to 150 parts of exciting agent, 5 to 10 parts of toughening fiber and 150 to 200 parts of water. According to the invention, the thermoplastic anticorrosive resin and the solid waste-based alkali-activated material are adopted as main cementing materials, so that the coating has the characteristics of short curing time, high early strength, acid and alkali corrosion resistance, water and oil corrosion resistance, high toughness and crack resistance, and is suitable for various corrosive environments; meanwhile, the solid waste is subjected to resource utilization, so that the cost is reduced, and secondary utilization of solid waste resources is facilitated.
本发明公开了一种超早强防腐砂浆及制备方法。本发明的超早强防腐砂浆,按重量份计,包括以下组分:防腐树脂400‑500份,增塑剂40‑50份,消泡剂1‑5份,憎水剂25‑35份,固废微粉200‑300份,尾矿砂200‑300份,激发剂100‑150份,增韧纤维5‑10份和水150‑200份。本发明采用热塑性防腐树脂和固废基碱激发材料作为主要胶凝材料,具有固化时间短,早期强度高、耐酸碱侵蚀、耐水油侵蚀、高韧性防裂的特点,适用于各种腐蚀性的环境中;同时由于对固废进行资源化利用,降低了成本,有利于推动固废资源二次利用。
Super-early-strength anticorrosive mortar and preparation method thereof
一种超早强防腐砂浆及其制备方法
ZHU YANCHAO (Autor:in) / CHENG FANGDI (Autor:in) / LUO SHUAISHUAI (Autor:in) / WANG JUNJIE (Autor:in) / ZHENG XINYI (Autor:in)
03.01.2025
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2023
|Anticorrosive interface treating mortar and preparation method thereof
Europäisches Patentamt | 2015
|Anticorrosive high-hardness mortar and preparation method thereof
Europäisches Patentamt | 2015
|Early strength coating mortar and preparation method thereof
Europäisches Patentamt | 2015
|