METHOD FOR PRODUCING -EUCRYPTITE FINE PARTICLES
Provided is a production method characterized in that a mixed solution containing water-soluble lithium salt, water-soluble aluminum salt, and colloidal silica in a molar ratio with respect to lithium atoms, aluminum atoms, and silicon atoms (Li:Al:Si) of 1:1:1 is dried by spraying in an atmosphere having a temperature of from 50°C to less than 300°C, and then the solution is fired in an atmosphere having a temperature of 600-1,300°C.
METHOD FOR PRODUCING -EUCRYPTITE FINE PARTICLES
Provided is a production method characterized in that a mixed solution containing water-soluble lithium salt, water-soluble aluminum salt, and colloidal silica in a molar ratio with respect to lithium atoms, aluminum atoms, and silicon atoms (Li:Al:Si) of 1:1:1 is dried by spraying in an atmosphere having a temperature of from 50°C to less than 300°C, and then the solution is fired in an atmosphere having a temperature of 600-1,300°C.
METHOD FOR PRODUCING -EUCRYPTITE FINE PARTICLES
VERFAHREN ZUR HERSTELLUNG FEINER EUCRYPTITPARTIKEL
PROCÉDÉ POUR PRODUIRE DES PARTICULES FINES DE BÊTA-EUCRYPTITE
KATO HIROKAZU (Autor:in) / ISAJI TADAYUKI (Autor:in) / KASHIMA YOSHIYUKI (Autor:in) / NAKAJIMA JUN-ICHI (Autor:in)
18.04.2018
Patent
Elektronische Ressource
Englisch
Synthesis of eucryptite spheres
British Library Online Contents | 2008
|Synthesis of eucryptite and eucryptite-zirconia composite powders using aqueous sol-gel technique
British Library Online Contents | 1997
|