Method for producing β-eucryptite fine particles
The β-eucryptite fine particle production method of the invention includes spraying, into an atmosphere at 50° C. to a temperature lower than 300° C., a solution containing a water-soluble lithium salt, a water-soluble aluminum salt, and colloidal silica, in such amounts that the mole proportions among lithium atoms, aluminum atoms, and silicon atoms (Li:Al:Si) are adjusted to 1:1:1, to thereby dry the solution, and, subsequently, firing the dried product in air at 600 to 1,300° C.
Method for producing β-eucryptite fine particles
The β-eucryptite fine particle production method of the invention includes spraying, into an atmosphere at 50° C. to a temperature lower than 300° C., a solution containing a water-soluble lithium salt, a water-soluble aluminum salt, and colloidal silica, in such amounts that the mole proportions among lithium atoms, aluminum atoms, and silicon atoms (Li:Al:Si) are adjusted to 1:1:1, to thereby dry the solution, and, subsequently, firing the dried product in air at 600 to 1,300° C.
Method for producing β-eucryptite fine particles
KATO HIROKAZU (Autor:in) / ISAJI TADAYUKI (Autor:in) / KASHIMA YOSHIYUKI (Autor:in) / NAKAJIMA JUN-ICHI (Autor:in)
19.03.2019
Patent
Elektronische Ressource
Englisch
Synthesis of eucryptite spheres
British Library Online Contents | 2008
|Synthesis of eucryptite and eucryptite-zirconia composite powders using aqueous sol-gel technique
British Library Online Contents | 1997
|