THICKENING SLAG MORTAR AND MANUFACTURING METHOD THEREOF
To provide a manufacturing method of thickening slag mortar that can maintain long usable time while reducing bleeding and material separation during pumping by instantaneously thickening.SOLUTION: A manufacturing method of thickening slag mortar that contains at least slag powder, gypsum powder, filler, water glass and water, does not contain cement, and is used by pumping includes a slag mortar making process in which water is added to slag powder, gypsum powder, and filler to make slag mortar and a water glass adding and stirring process in which, after adding water glass to slag mortar made in the slag mortar making process to generate floc-like heterogeneous gel, the floc-like heterogeneous gel is crushed and refined by stirring to promote gelation.SELECTED DRAWING: Figure 2
【課題】瞬時に増粘させて圧送時のブリーディングや材料分離を低減しつつ、可使時間を長時間持続できる増粘性スラグモルタルの製造方法を提供することを提供すること。【解決手段】スラグ粉末、石膏粉末、フィラー、水ガラス及び水を少なくとも含有し、セメントを含有せず、ポンプ圧送して使用される増粘性スラグモルタルの製造方法であって、スラグ粉末、石膏粉末及びフィラーに水を加えてスラグモルタルを生成するスラグモルタル生成工程と、前記スラグモルタル生成工程で生成したスラグモルタルに水ガラスを加えてフロック状の不均一ゲルを生成した後、撹拌して前記フロック状の不均一ゲルを砕いて微細化しながらゲル化を促進する水ガラス添加撹拌工程とを備える。【選択図】図2
THICKENING SLAG MORTAR AND MANUFACTURING METHOD THEREOF
To provide a manufacturing method of thickening slag mortar that can maintain long usable time while reducing bleeding and material separation during pumping by instantaneously thickening.SOLUTION: A manufacturing method of thickening slag mortar that contains at least slag powder, gypsum powder, filler, water glass and water, does not contain cement, and is used by pumping includes a slag mortar making process in which water is added to slag powder, gypsum powder, and filler to make slag mortar and a water glass adding and stirring process in which, after adding water glass to slag mortar made in the slag mortar making process to generate floc-like heterogeneous gel, the floc-like heterogeneous gel is crushed and refined by stirring to promote gelation.SELECTED DRAWING: Figure 2
【課題】瞬時に増粘させて圧送時のブリーディングや材料分離を低減しつつ、可使時間を長時間持続できる増粘性スラグモルタルの製造方法を提供することを提供すること。【解決手段】スラグ粉末、石膏粉末、フィラー、水ガラス及び水を少なくとも含有し、セメントを含有せず、ポンプ圧送して使用される増粘性スラグモルタルの製造方法であって、スラグ粉末、石膏粉末及びフィラーに水を加えてスラグモルタルを生成するスラグモルタル生成工程と、前記スラグモルタル生成工程で生成したスラグモルタルに水ガラスを加えてフロック状の不均一ゲルを生成した後、撹拌して前記フロック状の不均一ゲルを砕いて微細化しながらゲル化を促進する水ガラス添加撹拌工程とを備える。【選択図】図2
THICKENING SLAG MORTAR AND MANUFACTURING METHOD THEREOF
増粘性スラグモルタル及びその製造方法
OKADA KAZUNARI (Autor:in) / OYAMA SUSUMU (Autor:in) / MIYAKE SHINJI (Autor:in) / KATO MITSURU (Autor:in) / KOYAMA TAKASHI (Autor:in) / GOTO TAKASHI (Autor:in) / UCHIKAWA YUYA (Autor:in) / KANETAKA TETSUJI (Autor:in) / TOSHIDA YASUHARU (Autor:in)
12.03.2024
Patent
Elektronische Ressource
Japanisch
Dry-mixed mortar thickening agent and preparation method thereof
Europäisches Patentamt | 2022
|Dry-mixed mortar thickening agent and preparation method thereof
Europäisches Patentamt | 2020
|Mortar water-retaining and thickening material and preparation method thereof
Europäisches Patentamt | 2022
|Lithium slag-based thickening agent and preparation method thereof
Europäisches Patentamt | 2024
|