Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
METHOD FOR MANUFACTURING ECO-FRIENDLY NON-TOXIC WATER PERMEABLE BLOCK
The present invention relates to a method for manufacturing an eco-friendly non-toxic water permeable block, allowing easy manufacture of the eco-friendly non-toxic water permeable block which is excellent in water permeability, lacks decoloration or discoloration so that semi-permanent use is possible, thereby reducing repairing costs, contributes to underground water depletion prevention and tree growth stimulation, lacks a pollution problem due to cement usage, and has an air purification function. The present invention as described above includes the steps of: manufacturing color aggregate by coloring aggregate, prepared by pulverizing natural stone, with pigment; mixing and agitating the color aggregate, two-component polyurethane resin, and a hardening accelerator; inserting the agitated admixture of the color aggregate, the two-component polyurethane resin, and the hardening accelerator into a molding press to compression-mold the admixture into a water permeable block; form-removing the water permeable block molded at the molding press from the molding press; and curing the water permeable block removed from the molding press.
본 발명은 친환경 무독성 투수블록 제조방법에 관한 것으로, 투수성이 우수하고, 탈색이나 변색이 없어 반영구적인 사용이 가능하여 보수비용을 절감할 수 있으며, 지하수 고갈 방지 및 수목의 생육촉진에도 기여하면서 시멘트 사용으로 인한 오염의 문제가 없는데다가 공기정화 기능까지 갖추고 있는 친환경 무독성 투수블록을 용이하게 제조할 수 있는 것이다. 이러한 본 발명은, 자연석을 분쇄한 골재에 안료를 착색하여 칼라골재를 제조하는 단계와; 상기 칼라골재와 2액형 폴리우레탄 수지와 경화촉진제를 혼합하여 교반하는 단계와; 교반된 칼라골재, 폴리우레탄 수지 및 경화촉진제의 혼합물을 성형기에 투입하여 투수블록으로 가압 성형하는 단계와; 상기 성형기에서 성형된 투수블록을 성형기에서 탈형하는 단계와; 상기 성형기에서 탈형된 투수블록을 양생하는 단계를 포함한다.
METHOD FOR MANUFACTURING ECO-FRIENDLY NON-TOXIC WATER PERMEABLE BLOCK
The present invention relates to a method for manufacturing an eco-friendly non-toxic water permeable block, allowing easy manufacture of the eco-friendly non-toxic water permeable block which is excellent in water permeability, lacks decoloration or discoloration so that semi-permanent use is possible, thereby reducing repairing costs, contributes to underground water depletion prevention and tree growth stimulation, lacks a pollution problem due to cement usage, and has an air purification function. The present invention as described above includes the steps of: manufacturing color aggregate by coloring aggregate, prepared by pulverizing natural stone, with pigment; mixing and agitating the color aggregate, two-component polyurethane resin, and a hardening accelerator; inserting the agitated admixture of the color aggregate, the two-component polyurethane resin, and the hardening accelerator into a molding press to compression-mold the admixture into a water permeable block; form-removing the water permeable block molded at the molding press from the molding press; and curing the water permeable block removed from the molding press.
본 발명은 친환경 무독성 투수블록 제조방법에 관한 것으로, 투수성이 우수하고, 탈색이나 변색이 없어 반영구적인 사용이 가능하여 보수비용을 절감할 수 있으며, 지하수 고갈 방지 및 수목의 생육촉진에도 기여하면서 시멘트 사용으로 인한 오염의 문제가 없는데다가 공기정화 기능까지 갖추고 있는 친환경 무독성 투수블록을 용이하게 제조할 수 있는 것이다. 이러한 본 발명은, 자연석을 분쇄한 골재에 안료를 착색하여 칼라골재를 제조하는 단계와; 상기 칼라골재와 2액형 폴리우레탄 수지와 경화촉진제를 혼합하여 교반하는 단계와; 교반된 칼라골재, 폴리우레탄 수지 및 경화촉진제의 혼합물을 성형기에 투입하여 투수블록으로 가압 성형하는 단계와; 상기 성형기에서 성형된 투수블록을 성형기에서 탈형하는 단계와; 상기 성형기에서 탈형된 투수블록을 양생하는 단계를 포함한다.
METHOD FOR MANUFACTURING ECO-FRIENDLY NON-TOXIC WATER PERMEABLE BLOCK
친환경 무독성 투수블록 제조방법
CHOI YONG JU (Autor:in) / KIM DA YOUNG (Autor:in) / KIM YU BEOM (Autor:in) / CHOI YONG SEON (Autor:in)
25.07.2016
Patent
Elektronische Ressource
Koreanisch
IPC:
B28B
Formgeben von Ton oder anderen keramischen Stoffzusammensetzungen, Schlacke oder von Mischungen, die zementartiges Material enthalten, z.B. Putzmörtel
,
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG OR MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
/
B28C
Tonaufbereitung
,
PREPARING CLAY
/
C04B
Kalk
,
LIME
/
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
Europäisches Patentamt | 2024
|PERMEABLE BLOCK AND MANUFACTURING METHOD OF PERMEABLE BLOCK
Europäisches Patentamt | 2016
|