LIGHTWEIGHT GROUT COMPOSITION AND GROUTING METHOD THEREWITH
The present invention relates to a lightweight grout composition and a grouting method using the same. The lightweight grout composition of the present invention comprises: 10-60 wt% of Portland cement, 1-10 wt% of silicon wafer waste sludge solid-liquid separation dry substance, 10-60 wt% of air cooling dry bottom ash, 0.1-10 wt% of calcium sulfoaluminate, magnesium sulfoaluminate, or calcium aluminate, 0.1-10 wt% of anhydrous gypsum, gypsum hemihydrate, or gypsum dihydrate, 0.01-3 wt% of superplasticizer, 0.001-1 wt% of thickener, and 0.01-1 wt% of anti-foaming agent. The lightweight grout composition of the present invention: reduces fractures caused by compressive, bending, and tensile strengths thereof at early ages, especially by an expansion characteristic thereof at early ages by being mixed with the silicon wafer waste sludge solid-liquid separation dry substance; has improved acid proof and chloride invasion resistance by using dry bottom ash having pozzolanic reaction properties as a substitute for sand; and generates almost no material separation by having lower density than sand, and thus has better durability than a conventional grout composition, thereby being able to be used for preventing a tunnel, a common duct, a cutting surface of excavation, an inclined surface (or a slope), or soft ground from being eroded, or for preventing earth and sand from being swept away.
본 발명은 경량 그라우트 조성물 및 이를 이용한 그라우팅 시공방법에 관한 것이다. 경량 그라우트 조성물은 포틀랜드시멘트 10∼60 중량%, 실리콘 웨이퍼 폐슬러지 고액분리 건조물 1~10 중량%, 공랭식 건조 바텀애쉬 10~60 중량%, 칼슘설포알루미네이트 또는 마그네슘설포알루미네이트 또는 칼슘알루미네이트 0.1~10 중량%, 무수석고 또는 반수석고 또는 이수석고 0.1~10 중량%, 유동화제 0.01~3 중량%, 증점제 0.001~1 중량%, 소포제 0.01~1 중량%를 포함하여 이루어진다. 본 발명은 실리콘 웨이퍼 폐슬러지 고액분리 건조물을 혼입하여 초기 재령의 압축, 휨, 인장강도, 특히 팽창특성에 의한 균열저감의 특성을 부여하고, 포졸란 반응 특성이 있는 건조 바텀애쉬를 모래 대용으로 사용하여 내산 및 내염해성을 개선시키고, 모래보다 밀도가 낮아 재료분리가 거의 발생하지 않기 때문에 기존의 그라우트 조성물보다 내구성이 우수한 특성을 보유한, 터널, 공동구, 터파기 굴착면, 사면(또는 법면, 비탈면), 연약지반 등의 침식이나 토사의 유실을 방지하기 위하여 사용될 수 있다
LIGHTWEIGHT GROUT COMPOSITION AND GROUTING METHOD THEREWITH
The present invention relates to a lightweight grout composition and a grouting method using the same. The lightweight grout composition of the present invention comprises: 10-60 wt% of Portland cement, 1-10 wt% of silicon wafer waste sludge solid-liquid separation dry substance, 10-60 wt% of air cooling dry bottom ash, 0.1-10 wt% of calcium sulfoaluminate, magnesium sulfoaluminate, or calcium aluminate, 0.1-10 wt% of anhydrous gypsum, gypsum hemihydrate, or gypsum dihydrate, 0.01-3 wt% of superplasticizer, 0.001-1 wt% of thickener, and 0.01-1 wt% of anti-foaming agent. The lightweight grout composition of the present invention: reduces fractures caused by compressive, bending, and tensile strengths thereof at early ages, especially by an expansion characteristic thereof at early ages by being mixed with the silicon wafer waste sludge solid-liquid separation dry substance; has improved acid proof and chloride invasion resistance by using dry bottom ash having pozzolanic reaction properties as a substitute for sand; and generates almost no material separation by having lower density than sand, and thus has better durability than a conventional grout composition, thereby being able to be used for preventing a tunnel, a common duct, a cutting surface of excavation, an inclined surface (or a slope), or soft ground from being eroded, or for preventing earth and sand from being swept away.
본 발명은 경량 그라우트 조성물 및 이를 이용한 그라우팅 시공방법에 관한 것이다. 경량 그라우트 조성물은 포틀랜드시멘트 10∼60 중량%, 실리콘 웨이퍼 폐슬러지 고액분리 건조물 1~10 중량%, 공랭식 건조 바텀애쉬 10~60 중량%, 칼슘설포알루미네이트 또는 마그네슘설포알루미네이트 또는 칼슘알루미네이트 0.1~10 중량%, 무수석고 또는 반수석고 또는 이수석고 0.1~10 중량%, 유동화제 0.01~3 중량%, 증점제 0.001~1 중량%, 소포제 0.01~1 중량%를 포함하여 이루어진다. 본 발명은 실리콘 웨이퍼 폐슬러지 고액분리 건조물을 혼입하여 초기 재령의 압축, 휨, 인장강도, 특히 팽창특성에 의한 균열저감의 특성을 부여하고, 포졸란 반응 특성이 있는 건조 바텀애쉬를 모래 대용으로 사용하여 내산 및 내염해성을 개선시키고, 모래보다 밀도가 낮아 재료분리가 거의 발생하지 않기 때문에 기존의 그라우트 조성물보다 내구성이 우수한 특성을 보유한, 터널, 공동구, 터파기 굴착면, 사면(또는 법면, 비탈면), 연약지반 등의 침식이나 토사의 유실을 방지하기 위하여 사용될 수 있다
LIGHTWEIGHT GROUT COMPOSITION AND GROUTING METHOD THEREWITH
경량 그라우트 조성물 및 이를 이용한 그라우팅 시공방법
KIM SOO RYONG (Autor:in) / KWON WOO TECK (Autor:in) / KIM YOUNG HEE (Autor:in) / SHIN DONG GEUN (Autor:in) / PARK JEONG JUN (Autor:in) / LEE JONG RYUL (Autor:in) / LEE SUN MOK (Autor:in) / LEE DAE GEUN (Autor:in)
05.10.2016
Patent
Elektronische Ressource
Koreanisch
IPC:
C04B
Kalk
,
LIME
GROUT COMPOSITION FOR GROUND REINFORCEMENT AND GROUTING METHOD THEREWITH
Europäisches Patentamt | 2018
|Europäisches Patentamt | 2018
|GROUT FILLER AND GROUTING METHOD USING THE GROUT FILLER
Europäisches Patentamt | 2015
|