Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
ECO-FRIENDLY FINISHING COMPOSITION FOR PROTECTING SURFACE OF CONCRETE STRUCTURE AND METHOD FOR PROTECTING SURFACE OF CONCRETE STRUCTURE THEREWITH
The present invention relates to an eco-friendly finishing composition for protecting the surface of concrete and a surface protection method for concrete structures using the same. The composition comprises: 5-95 wt% of an inorganic binder; 1-40 wt% of fine aggregate; 0.01-50 wt% of a durability improvement agent; and 0.1-20 wt% of water, wherein the durability improvement agent comprises: 35-99 wt% of a mesh-structure acrylic emulsion; 0.1-35 wt% of acrylonitrile styrene; 0.01-30 wt% of acrylate-2-chloroethyl; and 0.01-20 wt% of polysulfide. The present invention provides excellent hardness characteristics, durability and self-healing properties and thus, can reduce costs related to repair and maintenance. Moreover, the present invention provides excellent resistance to material separation and is convenient to use in construction, and thus can reduce construction time, construction costs, and repair time.
본 발명은, 무기 바인더 5∼95중량%, 잔골재 1∼40중량%, 내구성능 개선 혼화제 0.01∼50중량% 및 물 0.1~20중량%를 포함하며, 상기 내구성능 개선 혼화제는 망상구조 아크릴 에멀젼 35∼99중량%, 아크릴로니트릴 스티렌(acrylonitrile styrene) 0.1∼35중량%, 아크릴산-2-클로로에틸 0.01∼30중량% 및 폴리설파이드 0.01∼20중량%를 포함하는 것을 특징으로 하는 콘크리트 표면 보호용 친환경 마감재 조성물 및 이를 이용한 콘크리트 구조물 표면보호공법에 관한 것이다. 본 발명에 의하면, 우수한 강도특성, 내구성 및 자기보수성능을 보유하여 공용기간 증가와 유지보수에 소요되는 비용을 절감할 수 있다. 또한, 재료 분리 저항성이 우수하고, 시공이 용이하여 시공기간이 단축되고 시공비의 절감과 보수기간의 단축이 가능하다.
ECO-FRIENDLY FINISHING COMPOSITION FOR PROTECTING SURFACE OF CONCRETE STRUCTURE AND METHOD FOR PROTECTING SURFACE OF CONCRETE STRUCTURE THEREWITH
The present invention relates to an eco-friendly finishing composition for protecting the surface of concrete and a surface protection method for concrete structures using the same. The composition comprises: 5-95 wt% of an inorganic binder; 1-40 wt% of fine aggregate; 0.01-50 wt% of a durability improvement agent; and 0.1-20 wt% of water, wherein the durability improvement agent comprises: 35-99 wt% of a mesh-structure acrylic emulsion; 0.1-35 wt% of acrylonitrile styrene; 0.01-30 wt% of acrylate-2-chloroethyl; and 0.01-20 wt% of polysulfide. The present invention provides excellent hardness characteristics, durability and self-healing properties and thus, can reduce costs related to repair and maintenance. Moreover, the present invention provides excellent resistance to material separation and is convenient to use in construction, and thus can reduce construction time, construction costs, and repair time.
본 발명은, 무기 바인더 5∼95중량%, 잔골재 1∼40중량%, 내구성능 개선 혼화제 0.01∼50중량% 및 물 0.1~20중량%를 포함하며, 상기 내구성능 개선 혼화제는 망상구조 아크릴 에멀젼 35∼99중량%, 아크릴로니트릴 스티렌(acrylonitrile styrene) 0.1∼35중량%, 아크릴산-2-클로로에틸 0.01∼30중량% 및 폴리설파이드 0.01∼20중량%를 포함하는 것을 특징으로 하는 콘크리트 표면 보호용 친환경 마감재 조성물 및 이를 이용한 콘크리트 구조물 표면보호공법에 관한 것이다. 본 발명에 의하면, 우수한 강도특성, 내구성 및 자기보수성능을 보유하여 공용기간 증가와 유지보수에 소요되는 비용을 절감할 수 있다. 또한, 재료 분리 저항성이 우수하고, 시공이 용이하여 시공기간이 단축되고 시공비의 절감과 보수기간의 단축이 가능하다.
ECO-FRIENDLY FINISHING COMPOSITION FOR PROTECTING SURFACE OF CONCRETE STRUCTURE AND METHOD FOR PROTECTING SURFACE OF CONCRETE STRUCTURE THEREWITH
콘크리트 표면 보호용 친환경 마감재 조성물 및 이를 이용한 콘크리트 구조물 표면보호공법
GIM HYUN YOU (Autor:in)
22.03.2017
Patent
Elektronische Ressource
Koreanisch
Europäisches Patentamt | 2017
|Europäisches Patentamt | 2018
|Europäisches Patentamt | 2018
|Europäisches Patentamt | 2019
|Europäisches Patentamt | 2020
|