An alumina-based sintered body includes 92 mass % to 96 mass % of Al in terms of an oxide, and at least three elements selected from Group II elements, one of the at least three elements being 1.90 mass % or more of Ba in terms of an oxide. The alumina-based sintered body includes the following phases in a grain boundary phase present between alumina crystal grains: a first crystal phase containing Si and at least one of the Group II elements, and a second crystal phase containing Al and at least one of the Group II elements. In X-ray diffraction of the alumina-based sintered body, the maximum relative intensity of the first crystal phase and the maximum relative intensity of the second crystal phase are both 2 or above relative to the maximum diffraction intensity of the alumina crystal.
SPARK PLUG
An alumina-based sintered body includes 92 mass % to 96 mass % of Al in terms of an oxide, and at least three elements selected from Group II elements, one of the at least three elements being 1.90 mass % or more of Ba in terms of an oxide. The alumina-based sintered body includes the following phases in a grain boundary phase present between alumina crystal grains: a first crystal phase containing Si and at least one of the Group II elements, and a second crystal phase containing Al and at least one of the Group II elements. In X-ray diffraction of the alumina-based sintered body, the maximum relative intensity of the first crystal phase and the maximum relative intensity of the second crystal phase are both 2 or above relative to the maximum diffraction intensity of the alumina crystal.
SPARK PLUG
YOKOYAMA YUTAKA (Autor:in) / TANAKA KUNIHARU (Autor:in) / ARAKI NOBUYOSHI (Autor:in) / KURONO HIROKAZU (Autor:in) / SAJI TOSHIMASA (Autor:in) / NOMURA YUSUKE (Autor:in) / ISASA JUMPEI (Autor:in)
15.02.2018
Patent
Elektronische Ressource
Englisch