On Detection Technologies of Pre-Stressed Duct Grouting Fullness
Aging and deterioration (such as weakening of concrete strength and loss of prestress) of various degree will inevitably happen to prestressed concrete beam in service. In making the prestressed concrete beam, it is of vital importance to ensure that the prestress tension is sufficient, duct grouting is compact enough and concrete pouring is in good quality. Otherwise, structure will deteriorate faster and safety hazard and even bridge collapse may ensue, causing considerable economic losses.
On Detection Technologies of Pre-Stressed Duct Grouting Fullness
Aging and deterioration (such as weakening of concrete strength and loss of prestress) of various degree will inevitably happen to prestressed concrete beam in service. In making the prestressed concrete beam, it is of vital importance to ensure that the prestress tension is sufficient, duct grouting is compact enough and concrete pouring is in good quality. Otherwise, structure will deteriorate faster and safety hazard and even bridge collapse may ensue, causing considerable economic losses.
On Detection Technologies of Pre-Stressed Duct Grouting Fullness
Advanced Materials Research ; 933 ; 71-75
21.05.2014
5 pages
Aufsatz (Zeitschrift)
Elektronische Ressource
Englisch
Device and method for improving grouting fullness of sleeve
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2023
|Pre-stressed duct grouting agent, and preparation and application methods thereof
Europäisches Patentamt | 2016
|Europäisches Patentamt | 2021
|Prefabricated concrete sleeve grouting fullness measuring device and working method thereof
Europäisches Patentamt | 2021
|