A platform for research: civil engineering, architecture and urbanism
To combat segregation mainly caused by excessive hydrogen content it is essential to avoid use either of considerable quantity of silicon for deoxidation of metal in furnace or of large additions of lime and bauxite during refining period; metal should not become overheated. (see also English translation in Stal in English n 10 Oct 1959 p 778-82)
To combat segregation mainly caused by excessive hydrogen content it is essential to avoid use either of considerable quantity of silicon for deoxidation of metal in furnace or of large additions of lime and bauxite during refining period; metal should not become overheated. (see also English translation in Stal in English n 10 Oct 1959 p 778-82)
Spotty segregation in low alloy steels
Pyatnistaya likvatsiya v nizkolegirovannykh stalyakh
Kiselev, A.A. (author)
Stal ; 19
1959
5 pages
Article (Journal)
Russian
© Metadata Copyright Elsevier B. V. All rights reserved.
Spotty segregation in low alloy steels
Engineering Index Backfile | 1959
|Effect of composition of chromium aluminum steels on susceptibility to spotty segregation
Engineering Index Backfile | 1961
|Effect of composition of chromium aluminum steels on susceptibility to spotty segregation
Engineering Index Backfile | 1961
|Characterisation of Segregation Band Distributions in Hot-Rolled Alloy Steels
British Library Online Contents | 2002
|Segregation in Advanced Steels
British Library Online Contents | 1999
|